Technique Equipment Parameters Design of Titanium & Titanium Alloys Oxidizing for Large Area and Batch-Type Production

Article Preview

Abstract:

Analyses the principal of titanium & titanium alloys oxidizing and the relation of thickness and color of the oxidizing film and the oxidizing power, The reasons are pointed out, which the low reapparition-rate and the difficult control of color of oxidizing film lie in titanium & titanium alloys anodizing with common power. The technique and equipment parameters are acquired by anodizing experiments, which ensure the identity of oxidizing film color of titanium & titanium alloys oxidizing for batch-type production, where the voltage is severed as a control object, the adjustable stable voltage and the controlling pattern of self-shutting are used, that enable the terminal voltage and the pattern of voltage inputting to be accurately controlled, and ensure the identity of oxidizing film color for batch-type production. These are utilitarian measures in the application of titanium & titanium alloys oxidizing for batch-type production.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 712-715)

Pages:

26-29

Citation:

Online since:

June 2013

Authors:

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Xiangming Tuo, Nan Li. Titanium and titanium alloy anode oxidation coloring layer structure and tensile properties [J].journal of rare metal, 1997.3

Google Scholar

[2] Hanmin Zhang. Titanium coloring oxidation technology [M]. Electroplating and precision decoration, P15, vol.14 no.4, 1992.7

Google Scholar