Study on the Crimp Property of PTT/PET Bicomponent Filament

Article Preview

Abstract:

In this work, the crimp properties of PTT/PET bicomponent filament with different component ratios were investigated. The results show that, after boiling water treatment for 15 minutes, the crimpability of 50/50 component ratio is superior to that of 40/60 and 60/40 component ratio. Heat treatment can realize the shrinkage difference of the two components in a biocomponent filament and enable the biocomponent filament to have good crimpability and bulkiness. In addition, different heat treatments, heat treatment time and heat treatment temperature can also bring different crimp effects to the biocomponent filaments.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 781-784)

Pages:

2680-2684

Citation:

Online since:

September 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] R. H. Brand and Stanely Backer: Textile Reaserch Journal, vol. 32 (1962), pp.39-49.

Google Scholar

[2] M. J. Denton: Journal of the textile institute, vol. 73 (1982), pp.253-263.

Google Scholar

[3] S. P. Rwei,Y. T. Lin, Y. Y. Su: Polymer Engineering and science, vol. 45 (2005), pp.838-845.

Google Scholar

[4] Jin Luo, Fumei Wang and Bugao Xu, Textile Reaserch Journal, vol. 81 (2011), pp.538-544.

DOI: 10.1177/0040517510383616

Google Scholar

[5] Mu Yao et al: Textile Materials (Textile Industry Press, Beijing 1980). (in Chinese).

Google Scholar

[6] Shu-jing Zhao: Experimental course for Textile Materials (China Textile Press, Beijing 1989). (in Chinese).

Google Scholar