Analysis and Control the Pressed into Defects of Acid Rolling Strip Foreign Body

Article Preview

Abstract:

There are two reasons to causes of defects of acid rolling line equipment and hot-rolled raw materials problems, so it is necessary to analyse the cold-rolled strip surface foreign body pressed into the defect microstructure and composition. It is found that this defect can be eliminated by improving the quality of the raw material, controlling strip shape, making reasonable squeezed roll transformation system, making the implementation of effective management of the full range of roll surface, carrying out the whole process of clean production, effectively controlling of the cold-rolled strip foreign body pressed into the generation of defects.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 785-786)

Pages:

1099-1103

Citation:

Online since:

September 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Feng Li, Xuewei Ye, Zhenglian Jiang. Identification and Control of Surface Defects on Cold Rolled Strip[J]. Metallurgical Equipment. 2010, (179): 65-69, In Chinese.

Google Scholar

[2] Feng Li, Xuewei Ye, Zhenglian Jiang. Analysis of the defect of impurity pressed in cold rolled sheet and its preventive measure[J]. Shanghai Metals. 2009, 31(2): 57-59, In Chinese.

Google Scholar

[3] Xingdong Peng, Lin Hu, Xiaodong Hu. Cold-rolled strip steel surface defect diagnosis[J]. Journal of University of Science and Technology Liaoning. 2010, 33(1), 24-28, In Chinese.

Google Scholar

[4] Jianjun Chu, Chang Liu, Qihong Xing. Analysis of Cause and Prevention Methods for the Impressed Extraneous Matter on Cold Rolling Steel Strip. Metallurgical Equipment. 2008, (169), 42-45, In Chinese.

Google Scholar