Preparation and Application of P-Mo-W Heteropoly Acid Catalyst
Abstract:
the phosphorus-molybdenum-tungsten heteropoly acid catalyst is prepared from such raw materials as phosphoric acid, sodium molybdate, sodium tungstate and characterized by infrared spectrum. Glyoxylic acid is prepared by catalytic oxidation of glyoxal in the presence of the self-prepared heteropoly acid catalyst and oxidizing agent hydrogen peroxide. The impact of catalytic reaction temperature, added catalyst, and use level of the hydrogen peroxide on the reaction for synthesizing the glyoxylic acid is investigated. The results show under such conditions as 4°C temperature, 0.15g catalyst, and 1.2:1 molar ratio of the hydrogen peroxide to the glyoxal, the phosphorus-molybdenum-tungsten heteropoly acid catalyst has higher catalytic activity and the mass fraction of the glyoxylic acid is 30%.
Info:
Periodical:
Pages:
2374-2378
Citation:
Online since:
November 2013
Authors:
Price:
Сopyright:
© 2014 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: