Processing Map of Mg-13Al-3Ca-3Zn-1Nd-0.2Mn Magnesium Alloy
Abstract:
Compression tests of Mg-13Al-3Ca-3Zn-1Nd-0.2Mn Magnesium alloy as-extruded had been performed in the compression temperature range from 200°C to 400°C and the strain rate range from 0.001 s−1 to 10 s−1 and the flow stress data obtained from the tests were used to develop the power dissipation map, instability map and processing map. The most unsuitable zones in the power dissipation map including 200°C - 315°C and 0.01s-1 - 0.1s-1 zone, 315°C - 400°C and 0.001s-1 - 0.01s-1 zone and 340°C - 360°C and 0.32 s-1 - 0.56 s-1 zone. The most unsuitable zones in the instability map are 310°C - 400°C, 0.001s-1 to 0.56 s-1 zone and 330°C - 400°C, 1s-1 to 10 s-1 zone. The most suitable temperature range is 330°C - 400°C and most optimal strain rate ranges are 1 s-1 - 10 s-1 and 0.001s-1 - 0.56 s-1.
Info:
Periodical:
Pages:
48-53
Citation:
Online since:
June 2014
Keywords:
Price:
Сopyright:
© 2014 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: