Thermal Shock Behaviour of Alumina-Mullite-Zircon Refractories

Abstract:

Article Preview

Info:

Periodical:

Key Engineering Materials (Volumes 264-268)

Main Theme:

Edited by:

Hasan Mandal and Lütfi Öveçoglu

Pages:

1747-1750

Citation:

C. Aksel "Thermal Shock Behaviour of Alumina-Mullite-Zircon Refractories ", Key Engineering Materials, Vols. 264-268, pp. 1747-1750, 2004

Online since:

May 2004

Authors:

Export:

Price:

$38.00

[1] C. Aksel: Materials Letters Vol. 57(4) (2002), p.992.

[2] C. Aksel: Ceramics International, Vol. 29(3) (2003), p.311.

[3] C. Aksel, M. Dexet, N. Logen, F. Porte, F.L. Riley and F. Konieczny: J. Eur. Ceram. Soc., Vol. 23(12) (2003), p. (2083).

[4] J.F. Shackelford, W. Alexander and J.S. Park: CRC Materials Science and Engineering Handbook, (CRC Press, Boca Raton, Florida 1994).

[5] Y. Shi, X.X. Huang and D.S. Yan: Ceramics International, Vol. 23(5) (1997), p.457.

[6] C. Aksel: Ceramics International Vol. 29(3) (2003), p.305.

[7] C. Aksel and F. Konieczny: Glass International, Vol. 24(1) (2001), p.16.

[8] K.J. Chen and Y.C. Ko: Am. Ceram. Soc. Bull., Vol. 62(9) (1983), p.1030.

[9] G. Orange, G. Fantozzi, F. Cambier, C. Leblud, M.R. Anseau and A. Leriche: J. Mat. Sci., Vol. 20 (1985), p.2533.

[10] S. Lathabai, D.G. Hay, F. Wagner and N. Claussen: J. Am. Ceram. Soc., Vol. 79(1) (1996), p.248.

[11] R.H.J. Hannink: J. Am. Ceram. Soc., Vol. 83(3) (2000), p.461.

[12] R. Stevens: Trans. J. Brit. Ceram. Soc., Vol. 80(3) (1981), p.81.

[13] British Standard Testing of Engineering Ceramics, BS 7134 Section 1. 2, (1989).

[14] ASTM C1161-90, Annual Book of ASTM Standards, Vol. 15. 01 (1991), p.327.

[15] ASTM D790M-86, Annual Book of ASTM Standards, Vol. 08. 01 (1988), p.290.

[16] W.F. Brown and J.E. Srawley: ASTM Spec. Tech. Publ., No: 410 (1967), p.1.

[17] D.P.H. Hasselman: Am. Ceram. Soc. Bull., Vol. 49(12) (1970), p.1033.

[18] P.S. Turner: J. Res. Natl. Bur. Stand., Vol. 37(4) (1946), p.239.

[19] A.A. Griffith: Philos. Trans. R. Soc., Vol. A221 (1920), p.163. 0 5 10 15 20 25 30 35 0 200 400 600 800 1000 1200 ∆∆∆∆T (°C) Strength (MPa) A B C 0 10 20 30 40 0 200 400 600 800 1000 1200 ∆∆∆∆T (°C) E (GPa) A B C.

Fetching data from Crossref.
This may take some time to load.