Fracture Strength of In-CeramTM Prostheses Fabricated by Double Sintering and Glass Infiltration

Article Preview

Abstract:

You might also be interested in these eBooks

Info:

Periodical:

Key Engineering Materials (Volumes 264-268)

Pages:

2067-2070

Citation:

Online since:

May 2004

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2004 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] E. A. McLaren, S.N. White: J Prosthet Dent Vol. 83 (2000), pp.216-222.

Google Scholar

[2] M. Sadoun: Proceedings of the 7 th International Symposium on Ceramics. Paris: (Quintessence Publishing Co, Paris, France 1988).

Google Scholar

[3] W.C. Wagner,T. M. Chu: J Prosthet Dent Vol. 76 (1996), pp.140-144.

Google Scholar

[4] R. A. Giordano, S. Campbell, R. Pober: J Prosthet Dent Vol. 73 (1995), pp.411-418.

Google Scholar

[5] M. Y. Wen, H. J. Mueller, J. Chai, W. T. Wozniak: Int J Prosthodont Vol. 12 (1999), pp.534-541.

Google Scholar

[6] R. Giordano, L. Pelletier, S. Campbell, R. Pober: J Prosthet Dent Vol. 73 (1995), pp.411-418.

Google Scholar

[7] VITA In-Ceram TM Alumina and VITA In-Ceram TM Sprint: Directions for Use Brochure (trademark of Vita Zahnfabrik H. Rauter GmbH & Co. ).

Google Scholar

[8] J. Tinschert , W. Mautsch, M. Augthun, H. Spiekermann: Int J Prosthodont Vol. 14 (2001), pp.231-238.

Google Scholar

[9] E. Helkimo, G. E. Carlsson, M. Helkimo: Acta Odontol Scand Vol. 35 (1977), pp.297-303.

DOI: 10.3109/00016357709064128

Google Scholar

[10] A. Waltimo, P. Kemppainen, M. Könönen: Scand J Dent Res Vol. 101 (1993), pp.416-421.

Google Scholar