Observation of Crack Originating from Non-Metallic Inclusions in Furnace-Induction Heated SUJ2 Steel under One-Point Rolling Contact Fatigue at High Contact Pressure

Article Preview

Abstract:

It is important to reveal the mechanism of crack growth from non-metallic inclusions because it commonly causes the origin of flaking fracture. In order to observe the cracks initiated from non-metallic inclusions under contact pressure, we performed one-point rolling contact fatigue tests using furnace-induction heated SUJ2 steel. We measured the hardness distribution of the furnace-induction heated (FIH) specimen and observed cracks with the inclusions at cross-sections.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volume 1033)

Pages:

3-7

Citation:

Online since:

June 2021

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2021 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] J. van der Geer, J.A.J. Hanraads, R.A. Lupton, The art of writing a scientific article, J. Sci. Commun. 163 (2000) 51-59. Reference to a book:.

Google Scholar

[2] W. Strunk Jr., E.B. White, The Elements of Style, third ed., Macmillan, New York, 1979. Reference to a chapter in an edited book:.

Google Scholar

[3] G.R. Mettam, L.B. Adams, How to prepare an electronic version of your article, in: B.S. Jones, R.Z. Smith (Eds.), Introduction to the Electronic Age, E-Publishing Inc., New York, 1999, pp.281-304.

Google Scholar

[4] R.J. Ong, J.T. Dawley and P.G. Clem: submitted to Journal of Materials Research (2003).

Google Scholar

[5] P.G. Clem, M. Rodriguez, J.A. Voigt and C.S. Ashley, U.S. Patent 6,231,666. (2001).

Google Scholar

[6] Information on http://www.weld.labs.gov.cn.

Google Scholar