Creep Behavior and Microstructures in Grain Boundary Strengthened Mg-Al-Ca Thixomolded® Alloys

Article Preview

Abstract:

The microstructures of thixomolded® (TM) Mg-Al-Ca alloys consist of α-Mg and eutectic compounds along grain boundaries. Misch metal (Mm) addition to TM Mg-Al-Ca alloys makes precipitates within α-Mg matrix and their number density and size depend on heat-treatment conditions. The small addition of Mm can keep the network-like grain boundary covering and the improvement of microstructure stability during creep. On the other hand, excessive Mm addition causes the deterioration of creep strength. The grain boundary coverage decreases with increasing Mm content due to the formation of coarse spherical Al-Mm based intermetallic compounds. Creep strength is significantly affected by both of the grain boundary coverage and the morphology of eutectic compounds along grain boundaries.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 706-709)

Pages:

1249-1254

Citation:

Online since:

January 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] S. Koike, K. Washizu, S. Tanaka, T. Baba and K. Kikawa, SAE Technical Paper (2000), 200-01-1117.

Google Scholar

[2] K. Y. Sohn, J. W. Jones, J. E. Allison: Magnesium Technology 2000, edited by H. I. Kaplan, J. N. Hryn and B. B. Clow, TMS (2000) p.271.

Google Scholar

[3] M. O. Pekguleryuz, J. Renaud: : Magnesium Technology 2000, edited by H. I. Kaplan, J. N. Hryn and B. B. Clow, TMS (2000) p.279.

Google Scholar

[4] ASM Speciality Handbook®, Magnesium and Magnesium Alloys, Edited by M. M. Avedesian, H. Baker, ASM International®, (1999), P. 14.

Google Scholar

[5] I. P. Moreno, T. K. Nandy, J. W. Joness, J. E. Allison and T. M. Pollock: Scr. Mater., Vol. 48 (2003), P. 1029.

Google Scholar

[6] A. Shibata, M. Suzuki, T. Tsukeda, K. Saito and K. Maruyama: J. Japan Inst. Metals, Vol. 70 (2006), P. 968 (in Japanese).

Google Scholar

[7] M. Suzuki, T. Tsukeda, K. Saito and K. Maruyama: 123rd Committee Report, Heat-Resistant Material, Japan Society for the Promotion oof Science, Vol. 45 (2004), P. 255 (in Japanese).

Google Scholar

[8] A. Suzuki, N. D. Saddock, J.W. Jones and T. M. Pollock: Scr. Mater., Vol. 51 (2004), P. 1005.

Google Scholar

[9] A. Suzuki, N. D. Saddock, J. W. Jones and T. M. Pollock: Acta Mater., Vol. 53 (2005), P. 2823.

Google Scholar

[10] K. Sakamoto and K. Yamamoto: J. Japan Inst. Light Met., Vol. 52 (2002), P. 437.

Google Scholar

[11] Binary Alloy Phase Diagrams 2nd ed., edited by T. B. Massalski, H. Okamoto, P. R. Subramainian and L. Kacprzak, ASM International, (1990).

Google Scholar

[12] M. C. Gao, A. D. Rollett and M. Widom: Calphad, Vol. 30 (2006), P. 341.

Google Scholar