Synthesis and Structural Characterization of La0.8Sr0.2MO3 (M=Mn, Fe, Co and Cr) Solid Ionic Material for Catalyst Application
Abstract:
La0.8Sr0.2MO3+δ, (M=Mn, Fe, Cr, Co) ceramics were prepared by using solid state reaction method. All raw materials were mixed and ground using mortar. Homogenized powders were calcined at 900°C for three hour followed by grounding and uniaxial pressed at 100MPa. Compacted pellets were further pressed using cold isostatic pressing machine at 2600kg/m.s and sintered at 1300°C with heating rate 5°C/min for 4 hour. Crystal structure and phase transformation of sintered samples were obtained using X-ray diffraction. Density and porosity are measured by using Archimedes principle. The morphology of sintered samples is observed using scanning electron microscopy, while elemental analysis using the EDX.
Info:
Periodical:
Pages:
48-51
Citation:
Online since:
January 2016
Keywords:
Price:
Сopyright:
© 2016 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: