The Structure of Coatings Obtained in the Zn-31Al-3Mg Bath on High-Silicon Steel

Article Preview

Abstract:

Coatings obtained in Zn-Al-Mg baths on steel plates by using the continuous method provide effective protection against corrosion. They have greater corrosion resistance than traditional zinc coatings. Even though Zn-Al-Mg coatings have many advantages, they are not made on galvanized products by use of the batch hot dip method. For products galvanized by use of the batch hot dip method coating growth mainly depends on the content of silicon in the steel. An increase in coating thickness is particularly intense in the case of high-silicon steel. In the paper the results of tests on obtaining Zn-Al-Mg coatings on high-silicon steel by use of the batch hot dip method have been presented. The growth kinetics of coatings obtained in the Zn-31Al-3Mg bath on steel with Si content of 0.27% has been defined. The structure has been developed and the chemical composition of particular structural components of the coating has be established. It has been determined that coatings obtained in the Zn-31Al-3Mg bath are continuous and they have uniform thickness. The structure of the coating is compact and the chemical composition points to the presence of phases of the Fe-Al system. The presence of silicon in the steel limits steel reactivity in the tested bath. The course of growth kinetics of the coating is close to parabolic.

You might also be interested in these eBooks

Info:

Periodical:

Solid State Phenomena (Volume 212)

Pages:

101-106

Citation:

Online since:

December 2013

Authors:

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] J. Pelerin, B. Bramaud, J.F. Nouville, D. Coutsouradis, D.C. Herrschaft, S.F. Radke, Proceedings of the 13th International Galvanizing Conference, London (1982) 49/I.

Google Scholar

[2] A.R. Borzillo, et al., Bethlehem Steel Corporation Japanese Patent 617971 (1971).

Google Scholar

[3] K. Nishimura, H. Shindo, K. Kato, Y. Morimoto, Microstructure and corrosion behavior of Zn-Mg-Al hot dip galvanized steel sheet, Proceedings of the 4th International Conference on Zinc and Zinc Alloy Coated Steel, GALVATECH, Chiba, Japan (1998).

DOI: 10.1520/a0653_a0653m-17

Google Scholar

[4] S. Tanaka, K. Honda, A. Takahashi, Y. Morimoto, M. Kurosaki, H. Shindo, K. Nishimura, M. Sugiyama, The performance of Zn-Al-Mg-Si hot-dip galvanized steel sheet, Proceedings of the 5th International Conference on Zinc and Zinc Alloy Coated Steel, GALVATECH, Brussels, Belgium (2001).

DOI: 10.2355/tetsutohagane1955.89.1_161

Google Scholar

[5] T. Tsujimura, A. Komatsu, A. Andoh, Influence of Mg content in coating layer and coating structure on corrosion resistance of hot-dip Zn-Al-Mg alloy coated steel sheet, Proceedings of the 5th International Conference on Zinc and Zinc Alloy Coated Steel, GALVATECH, Brussels, Belgium (2001).

DOI: 10.4028/www.scientific.net/amr.834-836.601

Google Scholar

[6] M. Volt, R. Bleeker, T. Maalman, E. van Perlstein, MagiZincTM: a new generation of hot-dip galvanized products, Proceedings of the Galvanized Steel Sheet Forum, ILZRO and IZA, Duesseldorf, Germany (2006).

Google Scholar

[7] P. Liberski, H. Kania, P. Podolski The structure and corrosion resistance of Zn-Al coatings obtained in batch double dip process, Physico Chemical Mechanics of Materials 5 (2006) 673-679.

Google Scholar

[8] J. Mendala, The influence of Si addition in 55AlZn bath on the coating structures obtained in the batch hotdip metallization, IOP Conf. Series: Materials Science and Engineering 22 (2011) 012005.

DOI: 10.1088/1757-899x/22/1/012005

Google Scholar

[9] J. Mendala, Influence of the cooling method on the structure of 55AlZn coatings, IOP Conf. Series: Materials Science and Engineering 22 (2011) 012004.

DOI: 10.1088/1757-899x/22/1/012004

Google Scholar

[10] H. Kania, Physico Chemical Mechanics of Materials 9 (2012) 496-500.

Google Scholar

[11] H. Kania, Development trends of hot dip galvanizing baths (in Czech), Konstrukce 6 (2012) P6-P15.

Google Scholar

[12] H. Kania, The structure of coatings obtained in the Zn-31Al-3Mg bath by the batch hot dip method, IOP Conf. Series: Materials Science and Engineering 35 (2012) 012003.

DOI: 10.1088/1757-899x/35/1/012003

Google Scholar

[13] H. Kania, The influence of Si content in steel on the growth kinetics and structure of hot dip Zn-31Al-3Mg coatings, The Book of Abstracts XIV Annual Conference YUCOMAT (2012) P.S.B. 19, 85.

Google Scholar