Fabrication of Antireflective Films Composed of High and Low Refractive Index Layers Using Layer-by-Layer Self-Assembly Method

Article Preview

Abstract:

We introduce a novel and versatile approach for controlling anti-reflective (AR) properties of multilayer films based on layer-by-layer (LbL) self-assembly (SA) method. For the fabrication of these films, blend (i.e., mixed) layers containing both polyanions (i.e., titanium precursor (TALH) and poly(sodium 4-styrenesulfonate) (PSS)) were assembled with polycation (i.e., poly(diallyldimethylammonium chloride) (PDAD)) for the formation of the high refractive index multilayers and on the other hand, the negatively charged silica particles with the diameter of about 100 nm were employed for low refractive index layer. The refractive index of TALH:PSS/PDAD multilayer was controlled by blending ratio and annealing temperature as TALH has the relatively high refractive index (n = 1.68) in comparison with that (n = 1.46) of conventional polyelectrolytes (PEs) at room temperature and furthermore these titanium precursors are partially changed into TiO2 with relatively high refractive indices (n = 1.50 ~ 1.81) at annealing temperature of 250 oC. In the case of silica particle layer used for low refractive index layer, the calculated refractive index was about 1.35 due to much vacancy among the adsorbed silica colloids although the inherent refractive index of silica material is about 1.45. As a result, the films composed of TALH:PSS/PDAD multilayers with tunable refractive index and silica colloidal layer can easily modulate the optical properties of multilayer films by blending ratio and heat treatment.

You might also be interested in these eBooks

Info:

Periodical:

Solid State Phenomena (Volumes 124-126)

Pages:

559-562

Citation:

Online since:

June 2007

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2007 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] M. Born and E. Wolf: Principles of Optics: Electromagnetic Theory of Propagation, Interference and Diffraction of Light (4th Edn., Pergamon, Oxford 1970).

Google Scholar

[2] M. S. Park, Y. Lee and J. K. Kim: Chem. Mater. Vol. 17 (2005), p.3944.

Google Scholar

[3] J. Hiller, J. D. Mendelsohn and M. F. Rubner: Nature Materials. Vol. 1 (2002), p.59.

Google Scholar

[4] T. Serizawa, S. Kmimura and M. Akashi: Colloids Surf. Vol. 164 (2000), p.237.

Google Scholar

[5] S. Lee, J. Drwiega, C. Y. Wu, D. Mazyck and W. M. Sigmund: Chem. Mater. Vol. 16 (2004), p.1160.

Google Scholar

[6] F. Caruso, X. Shi, R. A. Caruso and A. Susha: Adv. Mater. Vol. 13 (2001), p.740. 400 450 500 550 600 650 700 750 800.

Google Scholar

[93] [94] [95] [96] [97] [98] [99] 100 Transmittance (%) W avelength (nm ) ���� ����� ����� E 400 450 500 550 600 650 700 750 800.

Google Scholar

[93] [94] [95] [96] [97] [98] [99] 100 Transmittance (%) W avelength (nm ) ���� ����� ����� E 400 450 500 550 600 650 700 750 800.

Google Scholar

[93] [94] [95] [96] [97] [98] [99] 100 Transmittance (%) W avelength (nm) ���� ����� ����� D 400 450 500 550 600 650 700 750 800.

Google Scholar

[93] [94] [95] [96] [97] [98] [99] 100 Transmittance (%) W avelength (nm) ���� ����� ����� 400 450 500 550 600 650 700 750 800.

Google Scholar

[93] [94] [95] [96] [97] [98] [99] 100 Transmittance (%) W avelength (nm) ���� ����� ����� D.

Google Scholar