Abstract:
A high performance water resistance agent KD-3 prepared from OPC cement, fly ash, slag and additives was used for the modification of hemi-hydrate desulphurization gypsum. Various factors on gypsum block were investigated. The prepared gypsum block possesses excellent water-resistance, good operating property and high mechanical strength. The optimized results was obtained: calcined gypsum 74.9%, KD-3 25%, retarder 0.1%, curing temperature 60°C and curing time 16h.