Abstract:

In this paper we evaluated some surface characteristics of the Vacuum Aluminized Paper (VAP) to explore the ink adhesion on it. It is shown that this performance is quite unsatisfying due to the high gloss of the VAP which results in an even weaker surface energy than the surface tension of ink. The optimal drying time for the inked VAP under UV light with 125W of power is approximately 4.5 minutes, converts to the practical production, the printing speed of the VAP should be near to 7128 sheet/hour so as to fully solidify the UV ink thus acquires the optimal adhesion of ink.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

685-688

Citation:

Online since:

October 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] L.M. Wang, J. Wei and Q. Hu: Packaging Engineering, Vol. 25 (2004) No.6, pp.168-170 (in Chinese).

Google Scholar

[2] C.Y. Zhu: Shanghai Packaging, Vol. 18 (2002) No.6, pp.332-337 (in Chinese).

Google Scholar

[3] Y.J. Huang: Enterprise Standardization, (2007) No.5, p.50 (in Chinese)..

Google Scholar

[4] Z.W. Zhao: Printing Technology, (2000) No.8, pp.31-33 (in Chinese)..

Google Scholar

[5] Z.P. Hu: Shanghai Nonferrous Metals, Vol. 26 (2005) No.1, pp.32-33 (in Chinese)..

Google Scholar

[6] R.Q. Feng: Printing Principle and Technology (Graphic Communications Press, China 2005).

Google Scholar