Study of the Damage of Drills in Dry Drilling of NM360 Steels

Article Preview

Abstract:

According to the characteristics of NM360, a contrast experiment for drilling performance in YG8 cemented carbide twist drill, high-speed steel twist drill and factories used in coating the ordinary high-speed steel twist drill has been done. Using microscope to observe the damage of drills, we found that form this experiment some causation in tool invalidation that tool breakage is main factor for the high-speed steel drill bits, brittle fracture is main factor for carbide drill bits. Brittle carbide cutting tools, feed speed too much impact load is too large, causing the blade fracture. As the tool edge wedge angle is too small, poor edge strength, easy chipping, edge wedge angle can not be too small.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

275-278

Citation:

Online since:

December 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] China Machine Tool Business Network. Dry cutting tool and its design; http://www.jic35.cn/Tech_news/Detail/539.html

Google Scholar

[2] Hongfu Zhou . Machinery manufacturing technology base [J]. Beijing: Higher Education Press, 2004.3,48 to 49

Google Scholar

[3] Haiping Chang. Difficult to machine materials cutting tool material of choice [M]. Shanxi Machinery, September 2003, three (120), 57 to 58

Google Scholar

[4] Qifang Li . Difficult to machine materials processing technology [J]. Beijing: Beijing Science and Technology and Technology Press, 1992.4,1 ~ 2,171 ~ 202

Google Scholar

[5] Shigang Xiao. Tool materials and a reasonable choice [J]. Beijing: China Machine Press, (1981)

Google Scholar