Tribological Behavior of Si3N4-hBN Ceramic Materials Sliding against Fe-B Alloy without Lubrication

Article Preview

Abstract:

The tribological behavior of Si3N4-hBN composites sliding on Fe-B alloy without lubrication was investigated by using a pin-on-disc wear tester. The results showed that, the addition of hBN to Si3N4 could not effectively improve the tribological characteristics of Si3N4-hBN when it slid against Fe-B alloy. Without lubrication, the wear of Si3N4-hBN composites was resulted from cracking and fracture, while the hard phase Fe2B in Fe-B alloy spalled off during the friction test. So, high friction coefficients (>0.9) and high wear coefficients (>1×10-5mm3/Nm) were obtained.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

32-36

Citation:

Online since:

December 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Y.M. Gao, L. Fang, J.Y. Su:. Wear Vol. 210(1997), pp.1-7

Google Scholar

[2] X.Z. Zhao, J.J. Liu, B.L. Zhu, H.Z. Miao, Z.B. Luo: Ceramics International Vol. 23 (1997), pp.483-488

Google Scholar

[3] G. Akdogan, T.A. Stolarski: Ceramics International 29 (2003), pp.435-446

Google Scholar

[4] H.Czichos, D. Klaffke, E. Santner: Wear Vol. 190 (1995), pp.155-161

Google Scholar

[5] W. Chen, Y.M. Gao, C. Chen: Wear Vol. 269 (2010), pp.241-248

Google Scholar

[6] Z.L. Liu, Y.X. Li, X. Chen, K.H. Hu: Acta metallurgica sinica Vol. 43(2007), pp.477-481

Google Scholar

[7] H.G. Fu, Q. Xiao, J.C. Kuang: Materials Science and Engineering A Vol. 466(2007), pp.160-165

Google Scholar