Comparison of Oxidation Behavior of Binary Co-10X (x=Al, Si, Cr) Alloys at 973 and 1073K

Article Preview

Abstract:

Kinetics and products of oxidation behavior of binary Co-10Al, Co-10Si and Co-10Cr alloys at 0.1Mpa oxygen at 973 and 1073K were analyzed and compared. The investigations show that CoO doesn't provide protective properties at high temperatures. Among the three alloy components, Co-10Cr has better oxidation resistance at 973K, while Co-10Al has at 1073K, and the causes are given. In addition, the schematic model of scale growth process is presented.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

238-242

Citation:

Online since:

September 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] K. Przybylski, D. Szwagierczak, Oxi. Met. 17, 267 (1981).

Google Scholar

[2] I.G. Wright, G.C. Wood, Oxi. Met. 11, 163 (1977).

Google Scholar

[3] F.H. Stott, I.G. Wright, T. Hodgkiess, G.C. Wood, Oxi. Met. 11, 141 (1977).

Google Scholar

[4] G.N. Irving, J. Stringer, D. P. Whittle, Oxi. Met. 9, 427 (1975).

Google Scholar

[5] G. He, L.F. Jiao, H.T. Yuan, J. Electrochemistry Communications. 8, 1633 (2006).

Google Scholar

[6] Y. Wang, J.M. Lee, X. Wang, International journal of hydrogen energy. 35, 1669 (2010).

Google Scholar

[7] J.H. Xiang, L. Huang, H.H. Zhang, Advanced Materials Research, 284-286, 1546 (2011).

Google Scholar

[8] H.H. Zhang, J.H. Xiang, Y. Zhang, Journal of Northeastern University, 33, 212 (2012).

Google Scholar

[9] B. Gorr, S. Burk, V.B. Trindade, Oxi. Met. 74, 239 (2010).

Google Scholar

[10] S. Mrowec and K. Przybylski, Oxid. Met. 11, 365 (1977).

Google Scholar