Abstract:

In the trial, the author explores sodium nitrite, triethanolamine and sodium on fluidity initial and final setting time, flexural strength and compressive strength and other properties, of early strength reinforcement material. The results showed that, when sodium nitrite content is 0.2%, triethanolamine content is 0.05%, the dosage of sodium sulfate is 0.8%, final setting time for 58min, the initial flow greater than 320[mm], 30min flow greater than 280[mm], 2h compressive strength of 30[MPa], 1d bending greater than 10[MPa], 28d compressive strength greater than 90[MPa], on the early strength reinforcement, meet construction requirements.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

936-940

Citation:

Online since:

December 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Yu Aihong, Research of High Performance Concrete Admixture[D]. Shandong: Shandong Jianzhu University, 2001, 04.

Google Scholar

[2] Wen Guoliang, Yao Xueyan, Bai Meirong, With the analysis of cement concrete admixtures adaptability[J]. Concrete, 2010, 252(10): 82-83.

Google Scholar

[3] Yao Bingwen, Ding Qingjun, Mei Shigang, etc. New hardening accelerator affecting concrete properties[J]. Concrete, 2005, 191(9): 49-54.

Google Scholar

[4] Leng Da, Zhang Xiong, Shen Zhonglin, Effects of water reducing agent and hardening accelerating admixture on the performance of cement-baced grouting material[J]. New Building Materials, 2008, 11: 21-25.

Google Scholar

[5] Ma Huizhu, Li Zongqi. Ettringite Formation in concrete[J]. Building Science, 2007, 23(11): 105 -111.

Google Scholar