Investigation on the Tensile Strength of Treated and Untreated Woven Sugar Palm Fibre Reinforced Composites

Article Preview

Abstract:

Natural fibres offer environmental benefits such as biodegradable and can be obtained from renewable resources. However, there is lack of investigations done to characterize and compare different types and orientation done on the natural fibres. This paper determines the tensile strength of sugar palm fibres under various treatment processes. The composites were fabricated using woven sugar-palm fibre treated with alkali and acid and used epoxy resin as the matrices for the composite. The tensile test was done to determine the tensile strength of the composite and the surface morphological analysis was done using SEM. The results demonstrated that the composite with the alkali treated fibres produced higher tensile strength compared to untreated and acid treated fibres. With these properties, it shows that treated woven sugar-palm fibre composite can withstand high stress load during operation compared to untreated fibres reinforced composites.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

588-592

Citation:

Online since:

October 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] D. Bactiar, S. M. Sapuan and M.M. Hamdan, Flexural properties of alkaline treated sugar palm fibre reinforced epoxy composites, Int. J. of Auto and Mech. Eng., (2010) 79-90.

DOI: 10.15282/ijame.1.2010.7.0007

Google Scholar

[2] M.R. Ishak, Z. Leman, S.M. Sapuan, M.Y. Salleh and S. Misri, The effect of sea water treatment on the impact and flexural strength of sugar palm fibre reinforced composites, Int. J. of Mech. and Mtrls Eng., (2009) 316-320.

Google Scholar

[3] N.D. Saheb, and J.P. Jog, Natural fiber polymer composites: A review, Adv. in Polymer Tech., (1999) 351–363.

DOI: 10.1002/(sici)1098-2329(199924)18:4<351::aid-adv6>3.0.co;2-x

Google Scholar

[4] Y. Cao, S. Shibata and I. Fukumoto, Press forming short natural fibre-reinforced biodegredable resin : Effect of fibre volume and length on flexural properties, Polymer Testing, (2005) 1005 - 1011.

DOI: 10.1016/j.polymertesting.2005.07.012

Google Scholar

[5] Y. Li, Y.W. Mai, and L. Ye, Sisal fibre and its composites: A review of recent developments, Composites Sci. and Tech., (2000) 2037-(2055).

DOI: 10.1016/s0266-3538(00)00101-9

Google Scholar

[6] X. Li, L.G. Tabil and S. Panigrahi, Chemical Treatments of Natural Fiber for Use in Natural Fiber-Reinforced Composites: A Review, J. of Polymers and the Env., (2007), 25-33.

DOI: 10.1007/s10924-006-0042-3

Google Scholar

[7] M.A. Sawpan, K.L. Pickering and A. Fernyhough, Effect of various chemical treatments on the fibre structure and tensile properties of industrial hemp fibres, Composites : Part A, (2011) 888-895.

DOI: 10.1016/j.compositesa.2011.03.008

Google Scholar

[8] P.J. Herrera-Franco and A. Valadez-Gonzalez, Mechanical properties of continuous natural fibre-reinforced polymer composites, Composites Part A: App. Sci. and Manufacturing, (2004) 339-345.

DOI: 10.1016/j.compositesa.2003.09.012

Google Scholar

[9] D. Bachtiar, S.M. Sapuan and M.M. Hamdan, The effect of alkaline treatment on tensile properties of sugar palm, Mtrls and Design, 29 (2008) 1285–1290.

DOI: 10.1016/j.matdes.2007.09.006

Google Scholar

[10] A. Ticoalu, T. Aravinthan and F. Cardona, Experimental investigation into gomuti fibres/polyester composite, Proc. of 21st Australasian Conf. on Mech. of Struc. and Mtrl. (2011).

DOI: 10.1201/b10571-80

Google Scholar