Investigation of the Semisolid Rheological Characteristics of AZ91D Alloy

Article Preview

Abstract:

The semisolid shear rheological characteristic of AZ91D alloy were investigated. The results show that: during the shear rheological test at 570 °C, a critical shear stress and a maximum shear stress are happened. And with holding time increasing, the solid fraction decreasing and the solid particles distributing more uniformly, the rheological rate increases but the critical and maximum shear stress decrease. At last, based on rheological theory, a five-component rheological model of the semisolid AZ91D alloy is established, which is H1 - (N1 / H2) - (N2 / S).

You might also be interested in these eBooks

Info:

Periodical:

Pages:

742-746

Citation:

Online since:

January 2015

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2015 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Z. Fan. Inter. Mater. Rev., Vol. 47 (2002), p.49.

Google Scholar

[2] H. V. Atkinson. Proc. in Mater. Sci., Vol. 50(2004), p.341.

Google Scholar

[3] Liu Zheng, Zhang Kui, Zeng Xiaoqin. Magnesium alloys theory and its application. Metallurgical Industry Publications, China (2002).

Google Scholar

[4] Yoshizawa Se, Lv Xinyu, Wang Guohui, et al. Heat Treatment of Metals, Vol. 28(2003), p.8.

Google Scholar

[5] F. Czerwinski. Mater. Sci. and Eng.: A, Vol. 367(2004), p.261.

Google Scholar

[6] Yoshizawa Se, Q. F. Li, Z. J. Liu, et al. China J. of nonferrous metals, Vol. 13 (2003), p.1156.

Google Scholar

[7] S. Kleiner, O. Beffort, M. Fuchs, et al. Proceedings of the 7th S2P Advanced Semisolid Processing of Alloys and Composites, Tokyo, 2002, p.257.

Google Scholar

[8] Yuan Longyu. Rheological mechanics. Science Press, China (1986).

Google Scholar

[9] Lin Bainian. Rheology of Cast. Harbin Institute of Technology Press, China (1991).

Google Scholar

[10] S. M. Xing, D. B. Zeng, J. T. Shi, et al. Foundry, Vol. 50(2001), p.66.

Google Scholar