Multi-Layer Microstructure of Sol-Gel Barium Titanate Thin Films for Optical Waveguide Applications

Article Preview

Abstract:

— Barium titanate (BaTiO3) thin films are suitable for many application especially photonics. BaTiO3 thin films are deposited using spin coating with an optimum spin speed of 4500rpm. The samples are then characterized using XRD, AFM and SEM. The results of the XRD analysis showed that both the 5-and 10-coated layers are polycrystalline BaTiO3 with differences in terms of diffraction intensity, due to the number of layers. As for optical application, the surface roughness is the most crucial part. The number of layers of 5 and 10 have thickness of 2.927nm and 4.456nm RMS.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

136-140

Citation:

Online since:

November 2015

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2015 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] A. Von Hippel ,R.G. Breckenridge, F.G. Chesley, and L. Tisza: Ind. Eng. Chem. Vol. 38(1946), p.1097.

DOI: 10.1021/ie50443a009

Google Scholar

[2] Tuller H.L. and Avrahami. Y, Electroceramics in Encyclopedia of Smart Material,; edited by Schwartz M.M. (John Wiley & Sons), New York, (2002).

Google Scholar

[3] M. Zgonik, P. Bernasconi, M. Duelli, R. Schlesser, P. Gunter, M.H. Garrett, D. Rytz, Y. Zhu, and X. Wu, Phys. Rev. B 50, 5941(1994).

Google Scholar

[4] Ashutosh Mishra, Niyati Mishra: International Journal of Materials Science and Applications (2012)p.14.

Google Scholar

[5] M.W. Cole, R.G. Geyer : Mech. Mater. Vol 36 (2004), p.1017.

Google Scholar

[6] D. M. Gill, C. W. Conrad, G. Ford, B. W. Wessels, and S. T. Ho: Appl. Phys. Lett., Vol. 71(1997) p.1783.

Google Scholar

[7] O. Namsar, A. Watcharapasorn, S.: Ceramics International, 38S, S95–S99. (2012).

Google Scholar

[8] Ala'eddin A. Saif, P. Poopalan, Physica B: Condensed Matter, vol. 406 (2011) p.1283.

Google Scholar