Fabrication and Properties of Si3N4-SiC-C Refractory Composites

Article Preview

Abstract:

Si3N4-SiC-C refractory composites were prepared under the condition of 1450°C × 3h with electrofoging anthracite, Si3N4, SiC as the raw material and the modification emulsified bitumen as the binder. The effects of the silicon and silica fine powder additives on the compressive strength of Si3N4- SiC-C refractory composites were studied. The results indicated that adding an appropriate ratio range of silicon or silica fine powder in the composites both can improve the compressive strength of the material.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 105-106)

Pages:

119-122

Citation:

Online since:

April 2010

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2010 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] H. Park, H. E. Kim and K. Niihara: J. Eur. Ceram. Soc. Vol. 18 (1998), p.107.

Google Scholar

[2] P. Y. Brisson, H. Darmstadt, M. Fafard, et al. : Carbon. Vol. 44 (2006), p.1438.

Google Scholar

[3] N.K. Reddy, J. Mukerji: J. Am. Ceram. Soc. Vol. 74 (1991), p.1139.

Google Scholar

[4] F. Luo, D. M. Zhu, H. Zhang, et al.: Mater. Sci. Eng., A. Vol. 431 (2006), p.285.

Google Scholar

[5] Y. R. Hong, J. L. Sun, Z. H. Huang, et al.: Non-Oxide Compound Refractory (Metallurgical Industry Press, Beijing, China, 2003).

Google Scholar