Effect of High Temperatures on Microstructure of Repair Mortars Containing Artificial Aggregate Based on Sintered Ash

Article Preview

Abstract:

The research presented in this article is focused on analyzing of high temperature influence on behaviour and microstructure of polymeric-cement matrix based repair materials containing lightweight aggregates on the basis of sintered ash. Also admixtures and polymeric fibres were applied to obtain the required parameters. The study of microstructure and its changes was realized using SEM, XRD and DTA analytical methods. Maximum temperature of exposure environment of the tested mortars was 1000°C, while cooling of specimens was gradual.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

147-151

Citation:

Online since:

April 2015

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2015 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Serdar Aydın, Development of a high-temperature-resistant mortar by using slag and pumice, Fire Safety Journal, Volume 43, Issue 8, November 2008, Pages 610-617.

DOI: 10.1016/j.firesaf.2008.02.001

Google Scholar

[2] Tanyildizi Harun, Coskun Ahmet. An experimental investigation of bond and compressive strength of concrete with mineral admixtures at high temperature. Arab J Sci Eng 2008; 33(2B): 443–9.

Google Scholar

[3] Melichar, T., Bydžovský, J., Černý, V. Research and Development of Lightweight Repair Mortars with Focus on Their Resistance to High Temperatures. International Science Index, 2014, vol. 8(2014), no. 7, pp.760-763. ISSN: 1307- 6892.

Google Scholar

[4] Melichar, T., Bydžovský, J., Keprdová, Š. Study of parameters of new polymer- cement composites after exposure to extreme temperatures. Advanced Materials Research, 2014, vol. 1000(2014), no. 07, pp.81-84. ISSN: 1022- 6680.

DOI: 10.4028/www.scientific.net/amr.1000.81

Google Scholar