Study on Deformation and Damage of Single Crystal MgO by Micro-Scratch

Article Preview

Abstract:

Scratch experiments were performed on MgO (001) plane along different crystallographic orientations with the gradually increased forces to investigate the deformaton and damage of MgO. The normal and lateral forces during scratch, as well as the topography characteristics of the residual scratch along different crystallographic orientations were compared and analyzed. The cracks propagation around the scratch were studied. The patterns of cracks and scratches were found to be very different when scratching along different crystallographic orientations. The mechanism of cracks forming beside the scratches on single crystal MgO was discussed.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 126-128)

Pages:

940-945

Citation:

Online since:

August 2010

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2010 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Z. Dong, H. Huang, and R. Kang: Mater. Sci. Eng. A (2010) doi: 10. 1016/j. msea. 2010. 03. 037.

Google Scholar

[2] J.W. Kim and S.Y. Lee: Physica C: Superconductivity 421 (2005) 10-14.

Google Scholar

[3] Z.G. Dong, H. Huang, and R.K. Kang: Adv. Mater. Res. 76-78 (2009) 404-409.

Google Scholar

[4] Z.G. Dong, R.K. Kang, and Z.Y. Jia: Adv. Mater. Res. 389-390 (2009) 7-12.

Google Scholar

[5] C. Tromas, J.C. Girard, V. Audurier, et al.: J. Mater. Sci. 34 (1999) 5337-5342.

Google Scholar

[6] Y. Gaillard, C. Tromas, and J. Woirgard: Acta Mater. 51 (2003) 1059-1065.

Google Scholar

[7] M.M. Chaudhri: Philos. Mag. A 53 (1986) l55-l63.

Google Scholar

[8] M.M. Chaudhri and Y. Enomoto: Wear 233-235 (1999) 717-726.

Google Scholar

[9] R. Sivakumar, M.I. Jones, K. Hirao, et al.: J. Eur. Ceram. Soc. 26 (2006) 351-359.

Google Scholar

[10] I. Zarudi, L. Zhang, and Y.W. Mai: J. Mater. Sci. 31 (1996) 905-914.

Google Scholar

[11] V. Le Houerou, J.C. Sangleboeuf, S. Deriano, et al.: J. Non-Cryst. Solids 316 (2003) 54-63.

Google Scholar

[12] K. Li, Y. Shapiro, and J.C.M. Li: Acta Mater. 46 (1998) 5569-5578.

Google Scholar

[13] W. Kanematsu: Wear 256 (2004) 100-107. Fig. 8 Cracks pattern beside the scratches along (a).

Google Scholar

[100] (b).

Google Scholar

[110] and (c).

Google Scholar

[210] orientations on MgO (001).

Google Scholar