Characterization of Porous Anodic Aluminium Oxide Film on Aluminium Templates Formed in Anodizing Process

Abstract:

Article Preview

A porous anodic aluminium oxide (AAO) films were successfully fabricated on aluminium templates by using anodizing technique. The anodizing process was done in the mixed acid solution of phosphoric acid and acetic acid. The growth, morphology and chemical composition of AAO film were investigated. During the anodizing process, the growth of the oxide pores was strictly influenced by the anodizing parameters. The anodizing was done by varying the voltage at 70 V to 130 V and temperature from 5 °C to 25 °C. The electrolyte concentration was remaining constant. In this study, all the samples were characterized using scanning electron microscope (SEM) and X-ray diffraction (XRD) techniques. From this study, the optimum parameters to obtain porous AAO film with the mixture of phosphoric acid and acetic acid solution can be known.

Info:

Periodical:

Edited by:

Zainal Arifin Ahmad, Muhd Ambar Yarmo, Fauziah Haji Abdul Aziz, Dr. Meor Yusoff Meor Sulaiman, Badrol Ahmad, Khairul Nizar Ismail, Nik Akmar Rejab

Pages:

55-60

DOI:

10.4028/www.scientific.net/AMR.173.55

Citation:

A. W. Juyana and M. N. Derman, "Characterization of Porous Anodic Aluminium Oxide Film on Aluminium Templates Formed in Anodizing Process", Advanced Materials Research, Vol. 173, pp. 55-60, 2011