Research on High-Efficiency Oxygen Blowing Technology for Semi-Steel Steelmaking

Article Preview

Abstract:

To improve the production efficiency of converter smelting and keep stabled during refining in Panzhihua Steel, the original nozzle was optimized and industrial tests have been carried out. Results show that the optimized nozzle has a better metallurgical effect on the condition that corrosion of lining is normal, the average volume of oxygen and oxygen supply intensity were increased by 1040 m3/h and 0.27 m3/(t •min) respectively, oxygen consumption was reduced by 1.99m3/t, the blowing time was lowered by 1.06 minutes, TFe content in slag is 19.65%, which is 1.5 percentage point lower than that of the original one. So, a better dephosphorization effect was obtained and metal loss is controlled.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 361-363)

Pages:

650-654

Citation:

Online since:

October 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Wu Fengllin, Cai Fushi. Oxygen Lance design of BOF. Beijing: Metallurgy Industry Press, 1982: 51 - 200.

Google Scholar

[2] Cai Zhipeng. Spraying Gun Design of BOF[J]. Report from Institute of Chemical Metallurgy; Chinese academy of Sciences. Beijing: Institute of Chemical Metallurgy: 1962, 7-10.

Google Scholar

[3] Flinn R. Jet Penetration and Bath Circulation in the Basic Oxygen Furnace [J] Transaction of the Metallurgical Society of AIME, 1967, 239 (11):1776-1791.

Google Scholar