Preparation and Characterization of Epoxidized Natural Rubber

Article Preview

Abstract:

Epoxidized Natural Rubber is prepared with latex processing technology. The relationships of the epoxidation with the reaction times and temperature were investigated. The structure of ENR was characterized by Fourier transform-infrared spectroscopy (FIIR). It is found that, the by products, ring-open components increases with the reaction temperatures and the reaction times. It is found that as the level of epoxidation increased, the number of tetrahydrofuran ring increased.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 396-398)

Pages:

478-481

Citation:

Online since:

November 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Ng S.C , Gan, L. H. European Polymer Journal.17(11), 1073-1077 (1981).

Google Scholar

[2] Gelling I R; Tinker A J; Haidzer A. R. Journal of Natural Rubber Research. 6(1), 20. (1991)

Google Scholar

[3] Gelling I. R. Rubber Chemistry and Technology 58(1), 86-97 (1985).

Google Scholar

[4] Cook, S., Materials world. 17, 30 (2009).

Google Scholar

[5] Gelling I R, Tinker A J & Haidzer A. R. Journal of Natural Rubber Research. 6(1), 20 (1991).

Google Scholar

[6] Ng S.C & Gan, L. H. European Polymer Journa.l 17(11), 1073 (1981).

Google Scholar