Study on Basic Properties of Akund Fibers and Pretreatment Process

Article Preview

Abstract:

The need for fiber modification was described, and the principles about how the reagents act on the fibers was also shown, then a series of orthogonal experiments was designed, at last a comprehensive analysis and pictures about the surface of the fibers before treatment and after treatment from the microscope was finished, at last get the conclusion 50g/L friction-up reagent and 3% weight gain reagent is the best solution.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 482-484)

Pages:

1373-1379

Citation:

Online since:

February 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] GB 11951—89《Terms of Natural Textile Fiber》.

Google Scholar

[2] Information on http://baike.baidu.com/view/796339.htm.

Google Scholar

[3] W. Li,W. Fei;H.Hu; X. Li: Studies on Structure and Properties of Akund . Fibre Product Testing Bureau of China(In Chinese), 2011, (7): pp.80-83.

Google Scholar

[4] M. Zhang:Strcuture and Thermal Properties of Kapok.Journal of Zhongyuan University of Technology(In Chinese),2008,(19):pp.47-51.

Google Scholar

[5] D. Liu,J.Yu,W.Wang,Z.Xia:Refining Pretreatment of Jute Fibers.Journal of Advances In Textile Technology(In Chinese) ,2008,(2):pp.69-71.

Google Scholar

[6] Shanghai Textile Holding Company ,Cotton Spinning Handbook,China Textile Press,2004,p.29.

Google Scholar