Experimental Research on the Iron Separation from an Ultra Poor Iron Ore

Article Preview

Abstract:

Test was made on separating iron from a ultra-low-grade vanadium titanium magnetite ore by a process of tailing discarding at a coarser size,staged grinding and staged low intensity magnetic separation. The results show that when the raw ore is treated by permanent dry magnetic separator with low intensity magnetic separation at 12~0 mm size,qualified tailings of about 20% yield can be discarded.The coarse concentrate is grounded in two stages. With the first stage grinding size being 45% -200 mesh and the second stage,75% -200 mesh,and then treated by two stage low intensity magnetic separation.As a result,an iron concentrate with a TFe grade of 65.80%and an iron recovery of 47.74%can be achieved.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 535-537)

Pages:

746-749

Citation:

Online since:

June 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] JunHui Zhang, Yuan Zhang, Metal Mine, No.388, pp.60-62, October, 2008.

Google Scholar

[2] Wen Chen, Metal Mine, No.407, pp.55-59, May, 2010.

Google Scholar

[3] Fengjun Shao, China Mining, Vol.9, No.9, pp.71-73, September, 2009.

Google Scholar

[4] Huanxiang Ma, Modern Mining, No.413, pp.23-25, January, 2010.

Google Scholar

[5] Yumin Qin,Mining Metallurgy, Vol.15, No.3, pp.18-21, September,2006.

Google Scholar