Metal injection molding(MIM) is a high efficient and near net shape manufacturing technology, which is appropriate for parts of small size and complex shape. MIM provides a viable method to fabricate metal and metal matrix composites with discontinuous reinforcements, and micro metal injection molding (μMIM) is applied to manufacturing products at micro scale. The status of the research and development of MIM and μMIM are reviewed. Processes including mixing, injection molding and subsequent debinding and sintering are summarized. And technical characteristic, injection processing and application of μMIM are introduced. The disadvantages in mixing, injection molding and debinding processes limit MIM to fabricating components with small size, low precision and mechanical properties, and it is necessary to prevent the powder from reuniting and avoid any oxidation and impurity during μMIM process. Further investigations in these areas will give rise to being explored of full potential of MIM technology.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

100-104

Citation:

Online since:

December 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Chen ZH. Modern powder metallurgy technology. Beijing: Chemical Industry Press; 2007, 421-477.

Google Scholar

[2] Bose A. Net shaping concepts for tungsten alloys and composites. Powder Metall 2003; 46: 121–6.

Google Scholar

[3] Li Y P, Qu X H, Shun Z Z. The present state in research and development trend in industrialization of PIM W-Cu composites. Powder Metall Technol 2003; 21: 108-10.

Google Scholar

[4] Hu GX, Zhang LX, Fan YL, Li YH. Fabrication of high porous NiTi shape memory alloy by metal injection molding. Journal of materials processing technology 2008; 206: 395-9.

DOI: 10.1016/j.jmatprotec.2007.12.044

Google Scholar

[5] Thian E S, Loh N H, Khor K A. Ti-6Al-4V/HA composite feedstock for injection molding. Mater Lett 2002; 56: 522-32.

DOI: 10.1016/s0167-577x(02)00544-x

Google Scholar

[6] Khakbiz M, Simchi A, Bagheri R. Analysis of the rheological behaviour and stability of 316L stainless steel-TiC powder injection molding feedstock. Mater Sci Eng 2005; A407: 105-13.

DOI: 10.1016/j.msea.2005.06.057

Google Scholar

[7] Lin KH, Lin YC, Lin ST. Effects of reduction atmosphere and nano carbon powder addition on the deoxidization of injection molded aluminum nitride parts. Journal of materials processing technology 2008; 201: 701-5.

DOI: 10.1016/j.jmatprotec.2007.11.140

Google Scholar

[8] Kim S W, Suk M J, Kim Y D, Moon IH. Micrometalpowder injection molding of W-Cu nanocomposite powder. Met Mater Int 2005; 11: 205–8.

DOI: 10.1007/bf03027443

Google Scholar

[9] LI ML, LI YM, HE H, Li LJ. Tchenique of solvent debinding for water atomized stainless steel powder injection molding compacts. Materials Science and Engineering of Powder Metallurgy 2011; 16: 61-6.

Google Scholar

[10] Zhao LMg, Qu XH, He XB, Li SQ. Powder injection moulding of Ti-47. 5Al-2. 5V-1. 0Cr. Journal of University of Science and Technology Beijing 2008; 30: 1144-8.

Google Scholar

[11] Li K, Cui DW, Qu X H. Effect of solution treatment on the microstructure and properties of 0Cr17Mn11Mo3N steel prepared by metal powder injection molding. Transacitons of material and heat treatment 2007; 28: 58-61.

Google Scholar

[12] Chu K, Jia CC, Liang XB, Qu XH. Fabrication of the electronic package box preform of SiCP/Al composites by powder injection molding. Journal of University of Science and Technology Beijing 2007; 29: 470-4.

Google Scholar

[13] Qiao B, Shang F, Ding M, Li HQ, He YQ, Yang JM. Process of 316L stainless steel coarse powder by injection molding. Journal of Aeronautical Materials 2010; 30: 30-5.

Google Scholar

[14] Qiao B, Shang F, Li HQ. Injection molding process of Fe-Ni-Cu-C alloy. Journal of Aeronautical Materials 2007; 27: 45- 8.

Google Scholar

[15] Yang JM, He YQ, Li HQ, Qiao B, Chen JS. Friction and wear behavior of SiCP/Cu composite prepared by powder injection molding. Advanced Materials Research 2011; 314-316: 1083-6.

DOI: 10.4028/www.scientific.net/amr.314-316.1083

Google Scholar

[16] Yi JH, Shi WF. The technology of metal powder injection molding and its development. Mining and metallurgical 2001; 21: 4-8.

Google Scholar

[17] Li DX, Huang BY. The status in metal injection molding. Powder Metal Material Science and Engineering 2002; 7: 24-30.

Google Scholar

[18] Li DX, Li YM, Qu XH, Huang BY. Metal Injeciton Molding Binder. Materials Review 2000; 14: 36-9.

Google Scholar

[19] Xiao PA, Hu YQ, Liu JZ, Liu SH, Dai KL, Chen ZH. Gradient negative pressure hot defatting technology for powder injecting formation. China, 200610136879. 8[ P] 2007-06-06.

Google Scholar

[20] Li YM, Khalil KA, Huang BY. Compact Shape Retention for Metal Injection Molding 17-4PH Stainless Steel. Rare Metal Materials and Engineering 2005; 34 : 22-7.

Google Scholar

[21] Deng ZY, Li YM, Tang R, Li DX, Li SL, Huang BY, et al. Vacuum defatting and sintering integrated furnace. China, 03202704. 4[P]. 2003- 12-31.

Google Scholar

[22] Yin H Q, Qu XH. Fabrication of micro gear wheelsby micro-powder injection molding. Journal of University of Science and Technology Beijing 2008; 15: 480−3.

DOI: 10.1016/s1005-8850(08)60090-0

Google Scholar