Study on Flotation of Lead-Zinc Oxide Ore from Yunnan
Abstract:
With regard to a deep-extend oxidized refractory lead-zinc ore from Yunnan province, containing 4.55% Pb and 17.09% Zn, a test study was carried out. By adopting single-stage roughing, single-stage scavenging, two-stage cleaning in the flotation of lead oxide ores, and single-stage cleaning, single-stage cleaning in the reverse flotation of zinc oxide ores, bulk concentrate of lead and zinc containing 36.60% Pb, 19.63% Zn with the Pb recovery of 82.45%, zinc concentrate containing 36.52% Zn, 0.44%Pb with the Zn recovery of 73.18% were obtained in the closed circuit experiment.