Analysis of Macro-Performance of FA Ceramic Brick

Article Preview

Abstract:

In this work, MSWI (municipal solid waste incineration) fly ash is used as a blending in production of ceramic brick by taking advantage of its high contents of SiO2, Al2O3 and CaO. Besides, macro-performance of the product was studied. It is found that when 20% fly ash is added, the product registers a high compressive strength of 18.9 MPa and a low water absorption of 8.9 % after being sintered at 1000°C. These results as a whole suggest that the use of MSWI fly ash in ceramic brick constitutes a potential means of adding value.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

279-282

Citation:

Online since:

November 2013

Authors:

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] D.S. Kosson, H.A.: J. Hazard. Mater. Vol. 47 (1996), pp.43-75.

Google Scholar

[2] J.P. Young, J. Heo.: J. Harzard. Mater. Vol. 91 (2002), pp.83-93.

Google Scholar

[3] D.Z. Chen, H.S. Zhang: Shanghai Environmental Sciences. Vol. 21 (2002), pp.344-349.

Google Scholar

[4] T. Mangialardi: J. Hazard. Mater. Vol. 87 (2001), pp.225-239.

Google Scholar

[5] GB 5086. 2: Solid waste-Extraction procedure for toxicity of solid waste-Horizontal vibration method (2007).

Google Scholar

[6] D.S. Kosson, V.D. Sloot: The Netherlands: Elsevier Science B.V. (1991).

Google Scholar

[7] H. Zhang: Tongji University, Shanghai (2003).

Google Scholar

[8] C.S. Kerby, J.D. Rimstidt: Environ, Sci. Technol. Vol. 27(1993), 652-660.

Google Scholar