Effect of Dielectric Properties and Elastic Strain Behavior on x/65/35 PLZT Ceramics in Lanthanum (x) Ions Contents

Article Preview

Abstract:

In this paper the effect of lanthanum addition on the phase formation, dielectric and ferroelectric characteristics of x/65/35 PLZT. This ceramics were prepared using mixed-oxide synthetic route via a rapid vibro-milling method. All samples were sintered at 1200°C for 12 h. X-ray diffraction was used to observe the crystal structure. It was found that when increasing lanthanum content, the structure remained rhombohedral. It can be seen that the change of behavior to ferroelectric relaxor with the increasing of lanthanum content resulted in the change of elastic strain

You might also be interested in these eBooks

Info:

Periodical:

Pages:

115-118

Citation:

Online since:

June 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] G.H. Heartling, Hot pressed (Pb, La)(Zr, Ti)O3 ferroelectric ceramics for electro-optic application, J. Am. Ceram. Soc. (1971) 1-11.

Google Scholar

[2] K.H. Härdtl, and D. Hennings, J. Am. Ceram. Soc. 55 (1972), 230.

Google Scholar

[3] A. Pelaiz Barranco, A. Huanosta Tera, R. Valenzuela Monjaras, J. Antonio Eiras, D. Garcia, F. Calderon Pinar, O. Perez Martinez, Influence of synthesis process on the AC response of PLZT (8/65/35) ferroelectric ceramics, J. Eur. Ceram Soc. 23 (2003).

DOI: 10.1016/s0955-2219(02)00288-1

Google Scholar

[4] G.H. Heartling, Ferroelectric Ceramic: History and Technology, J. Am. Ceram. Soc., (1999) 797-816.

Google Scholar

[5] E. Breval, M. Klimkiewicz, C. Wang and J.P. Dougherty, Annealing of sintered Pb0. 9175La0. 055Zr0. 775Ti0. 025O3 in air, J. Am. Ceram. Soc. 90 (2007) 2664-2666.

Google Scholar

[6] L. Chumprasert, A. Limpichaipanit, K. Chokethawai, S. Ananta and A. Ngamjarurojana, Effect of soaking time on phase formation and electrical properties of PLZT based ceramics, Ferroelectrics 208-209 (2013) 16-32.

DOI: 10.1080/00150193.2013.846752

Google Scholar

[7] M. Cerqueira, R.S. Nasar, E.R. Leite, E. Longo, and J.A. Varela, Synthesis and characterization of PLZT (9/65/35) by the Pechini method and partial oxalate, Mater. Lett. 35 (1998) 166-171.

DOI: 10.1016/s0167-577x(97)00240-1

Google Scholar

[8] V. Priyadarsini, P.V. salija, A.S. Divya and V. Kumar, Influence of strontium substitution on ferroelectric-relaxor transition in PLZT (7/60/40), J. Am. Ceram. Soc. 93 (2010) 3854-3586.

DOI: 10.1111/j.1551-2916.2010.04115.x

Google Scholar