Experimental Study on Factors Affecting the Generation of Ferrous Sulfide

Article Preview

Abstract:

Now steam stimulation gradually become one of the major thermal recovery methods, and hydrogen sulfide appears in the well casing. With the increase of the thermal recovery time and the application of SAGD technology, the number of wells containing hydrogen sulfide increased, and concentration of hydrogen sulfide are also rising,Producing corrosion products - ferrous sulfide. Ferrous sulfide has pyrophoric. When ferrous sulfide in contact with oxygen in the air can cause spontaneous combustion at room temperature. In order to avoid the occurrence of spontaneous combustion of ferrous sulfide we had an in-depth study of the spontaneous combustion of ferrous sulfide. Through laboratory tests we found the following points. At room temperature,sulfurization reaction of H2S gas and iron oxides occurs more easily in a dry environment. Temperature, H2S humidity, various iron oxides,have important effects on the generation of iron sulfide.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 986-987)

Pages:

76-79

Citation:

Online since:

July 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Yee H C. Construction of explicit and implicit symmetric TVD scheme and their applications[J]. JcompPhys, 1987, (68): 151-179.

DOI: 10.1016/0021-9991(87)90049-0

Google Scholar

[2] M. Hurchings. A model for the erosion of metals by spherical particles at normal incidence[J]. Wear, 1981(70): 269-281.

DOI: 10.1016/0043-1648(81)90347-1

Google Scholar

[3] Tilly G P. A two stage mechanism of ductile erosion[J]. Wear, 1973(23): 87-96.

DOI: 10.1016/0043-1648(73)90044-6

Google Scholar

[4] Bitter J G. A study of erosion phenomena[J]. Wear, 1983(6): 5-21.

Google Scholar

[5] FinnieⅠ. Stevick G R, Ridgely J R. The influence of impingement angle on the erosion of ductile metals by angular abrasive particles[J]. Wear, 1992(152): 91-98.

DOI: 10.1016/0043-1648(92)90206-n

Google Scholar