Morphology Control of High Luminance Phosphors

Article Preview

Abstract:

We report synthesis of well-grown blue phosphor powder, CaMgSi2O6:Eu2+, from new vapor phase method (Flash creation method) derived nanopowder precursor. Single phase phosphor sample was obtained by post-annealing at 1100 oC. Luminescence properties were compared with that of the sample synthesized by a conventional solid state reaction. The post-annealed sample showed intense blue emission under UV excitation.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

107-110

Citation:

Online since:

September 2008

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2009 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] S. Ekambaram and K. C. Patil, J. Alloys and Compd., 248, 7-12 (1997).

Google Scholar

[2] B. Howe and A. L. Diaz, J. Lumin., 109, 51-59 (2004).

Google Scholar

[3] T. Kunimoto, R. Yoshimatsu, K. Ohmi, S. Tanaka, and H. Kobayashi, IEICE Trans. Electron., E85-C, 1888-1894 (2002).

Google Scholar

[4] I-H. Jung, S. A. Decterev and A. D. Pelton, J. Euro. Ceram. Soc., 25, 313-333 (2005).

Google Scholar

[5] A. Watanabe, T. Fukui, K. Nogi, Y. Kizaki, Y. Noguchi and M. Miyayama, J. Ceram. Soc. Japan, 114, 97-101 (2006).

Google Scholar

[6] W. B. Kim, Y-I. Kim, J. H. Kang, D. Y. Jeon, H. K. Jung and K. Y. Jung, J. Mater. Res., 20, 2061-2066 (2005).

Google Scholar

[7] Phosphor Handbook. -2nd ed., Ed. by W. M. Yen, S. Shionoya and H. Yamamoto, CRC Press. -------------------- e-mail: ktoda@eng. niigata-u. ac. jp, fax: +81-25-262-6771, 200 300 400 500 0 100 200 Intensity / a. u. Wavelength / nm Post-annealed FCM sample Solid state reaction sample Fig. 4 Excitation (dashed line) and emission (solid line) spectra of the CMS powder synthesized by conventional solid state reaction (1200 o C) and post-annealing (1100 o C) of nano-precursor.

Google Scholar