Synthesis and Properties of Composite Stabilized ZrO2

Article Preview

Abstract:

Through Mechanical grounding method, CaZrO3 – 8YSZ(8% in mol yttria stabilized zirconia) electrolyte samples with different amounts of CaZrO3 at 10wt%, 20wt%, 30wt% were sintered at different temperatures in Muffle furnace. The decomposition temperature of CaZrO3 is 825°C-900°C under one atmosphere. At high temperature, CaZrO3 decomposes into CaO and ZrO2. So Y2O3-CaO-ZrO2 complex is composed. The effects of the sintering temperature and the contents of the CaZrO3 on the conductivity, porosity, flexure strength, hardness were investigated. XRD and SEM were used to analyse the compositions and microcosmic morphology.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

68-71

Citation:

Online since:

March 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] W.S. Lee, S.W. Kim, Synthesis and microstructure of Y2O3-doped ZrO2–CeO2 composite nanoparticles by hydrothermal process, J. Colloids and Surfaces A: Physicochem. Eng. Aspects. 313–314 (2008) 100–104.

DOI: 10.1016/j.colsurfa.2007.04.079

Google Scholar

[2] Z.P. Xie, Structural Ceramics , first ed., Tsinghua University Press, (2011).

Google Scholar

[3] M. Boulouz, L. Martin, A. Boulouz, A. Boyer, Effect of the dopant content on the physical properties of Y2O3–ZrO2 and CaO – ZrO2 thin films produced by evaporation and sputtering techniques, J. Materials Science and Engineering. B67 (1999).

DOI: 10.1016/s0921-5107(99)00338-4

Google Scholar