Strength and Behaviour of Small-Scale Reinforced High Calcium Fly Ash Geopolymer Concrete Beam with Short Shear Span

Article Preview

Abstract:

The small-scale reinforced high calcium fly ash geopolymer concrete beams with short shear span were studied in this research. Reinforced concrete beams with 150x150 mm2 cross-section and 530 mm in length were used for tests. Conventional reinforced Portland cement concrete beams (RC) with designed concrete compressive strengths of 35, 45 and 55 MPa and high-calcium fly ash geopolymer reinforced concrete beams with similar strength were tested. The geopolymer concretes (GC) were designed with alkaline liquid to fly ash ratio (L/A) of 0.5, sodium silicate to sodium hydroxide (S/H) ratio of 1.0 and two sodium hydroxide (NaOH) concentrations of 10M and 15M. Two temperatures of 23 and 60 °C were used for curing geopolymer reinforced concrete (GRC) beams for 24 hr, while RC beams were moist cured at 23 °C. The maximum sustained moment and shear were compared with the predicted values from the RC-design standard. The results showed that the failure patterns of small GRC beams were different to that of normal RC beam. The small GRC beams failed in flexure whereas the similar small RC beams failed in shear. However, the GRC beams were able to sustain higher shear and moment than the values obtained from the design code. The different in failure mechanism was probably due to the different in modulus of elasticity of geopolymer concrete and normal concrete.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

191-195

Citation:

Online since:

November 2016

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2017 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] J. A. Fernandez, L. I. Garcia, A. Palomo, Durability of alkali-activated fly ash cementitious materials, J Mater Sci. 42 (2007) 3055-65.

DOI: 10.1007/s10853-006-0584-8

Google Scholar

[2] P. Chindaprasirt, T. Chareerat, W. Kunawanakit, Geopolymer from mae moh fly ash, KKU En. J. 32 (2005) 715-24.

Google Scholar

[3] D. Hardjito, B.V. Rangan, Development and properties of low-calcium fly ash-based geopolymer concrete, Perth, Curtin University of Technology, Australia, (2005).

Google Scholar

[4] M.D.J. Sumajouw, B.V. Rangan, Low-Calcium Fly Ash-Based Geopolymer Concrete: Reinforced Beams and Columns, Perth, Curtin University of Technology, Australia , (2006).

Google Scholar

[5] C.K. Madheswaran, Ambily PS, Lakhsmanan N, Dattatreya JK, Jaffer Sathik SA, Shear behavior of reinforced geopolymer concrete thin webbed t-beams, ACI Mater. J. 111 (2014) 89-98.

DOI: 10.14359/51686449

Google Scholar

[6] T. Sugama, L.E. Brothers, Putte TRVd. Acid-resistant cements for geothermal wells: sodium silicate activated slag/fly ash blends, Advances in Cement Research, 2005. pp.65-75.

DOI: 10.1680/adcr.2005.17.2.65

Google Scholar

[7] P. Chindaprasirt, T. Chareerat, V. Sirivivatnanon, Workability and strength of coarse high calcium fly ash geopolymer, Cement Concrete Comp. 29 (2007) 224-9.

DOI: 10.1016/j.cemconcomp.2006.11.002

Google Scholar

[8] U. Rattanasak, P. Chindaprasirt, Influence of NaOH solution on the synthesis of fly ash geopolymer, Miner Eng. 22 (2009) 1073-8.

DOI: 10.1016/j.mineng.2009.03.022

Google Scholar

[9] P. Chindaprasirt, T. Chareerat, S. Hatanaka, T. Cao, High-strength geopolymer using fine high-calcium fly ash, J. Mater. Civ. Eng. 23 (2010) 264-70.

DOI: 10.1061/(asce)mt.1943-5533.0000161

Google Scholar

[10] J. Wongpa, K. Kiattikomol, C. Jaturapitakkul, P. Chindaprasirt, Compressive strength, modulus of elasticity, and water permeability of inorganic polymer concrete, Mater. Des. 31 (2010) 4748-54.

DOI: 10.1016/j.matdes.2010.05.012

Google Scholar

[11] K. Somna, C. Jaturapitakkul, P. Kajitvichyanukul, P. Chindaprasirt, Immobilization of heavy metals by fly ash-based geopolymer. KKU Res. J. 13 (2008) 1191-8.

DOI: 10.1016/j.fuel.2011.01.018

Google Scholar

[12] N.P. Topark, P. Chindaprasirt, V. Sata, Setting Time, strength, and bond of high-calcium fly ash geopolymer concrete, J. Mater. Civ. Eng. 27 (2014) 04014198.

DOI: 10.1061/(asce)mt.1943-5533.0001157

Google Scholar

[13] W. Prachasaree, S. Limkatanyu, A. Hawa, A. Samakrattakit, Development of equivalent stress block parameters for fly-ash-based geopolymer concrete, Arab. J. Sci. Eng. 39 (2014) 8549-58.

DOI: 10.1007/s13369-014-1447-2

Google Scholar

[14] P. Kong, B.V. Rangan, Shear Strength of High-Performance Concrete Beams. ACI. S. J. 95 (1998) 677-88.

Google Scholar

[15] K.H. Yang, H.S. Chung, E.T. Lee, H.C. Eun, Shear characteristics of high-strength concrete deep beams without shear reinforcements. Eng. Struct. 25 (2003) 1343-52.

DOI: 10.1016/s0141-0296(03)00110-x

Google Scholar

[16] W. Joost, L. Norbert, Size Effects in Short Beams Loaded in Shear. Structural Journal. 91 (1994).

Google Scholar

[17] G. Kani, How Safe are Our Large Reinforced Concrete Beams?. ACI. J. P. 64 (1967) 128-40.

DOI: 10.14359/7549

Google Scholar