Effects of Cu Addition on Age Hardening Response of Al-7Si-4Mg Alloys at 130 °C

Article Preview

Abstract:

The effects of Cu addition of 0.38, 3.82, and 6 wt. % in Al-7Si-4Mg alloy on hardness and age hardening response were discussed. Samples were solution treated at 495 °C for 2 h, quenched, and aged at 130 °C for 0 to 498 h. Characterization included hardness test, microstructural observation by an optical microscope (OM) and Scanning Electron Microscope (SEM) combined with Energy Dispersive X-Rays Spectroscopy (EDX), as well as Simultaneous Thermal Analysis (STA) testing. The results showed an increased in as-cast hardness along with addition of Cu. Peak hardness increased to 64.47, 65.8, and 70.1 HRB by addition of 0.38, 3.82, and 6 wt. % Cu, respectively. The addition of Cu promoted the formation of Al2Cu and Al5Cu2Mg8Si6 which contributed to higher as-cast hardness. Formation of GP-zone, θ”, and θ’ was observed after ageing at 48, 240, and 290 °C, respectively and no effects of Cu was detected on the formation temperatures of the precipitates.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

74-79

Citation:

Online since:

March 2020

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2020 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] http://energitoday.com/2014/04/01/kebutuhan-listrik-indonesia-tumbuh-84-per-tahun/, access-ed in May 1, (2018).

Google Scholar

[2] Jorstad, J., and Rasmussen, W. (2001). Aluminum Casting Tchnology Second Edition . Illinois: The American Foundrymen's Society, Inc.

Google Scholar

[3] J. Kaufman, and E.L. Rooy. (2004). Aluminum Alloy Casting: Properties, Processes, and Applications. Ohio: ASM International.

Google Scholar

[4] M. Syahid, B.T. Sofyan, S. G. Basuki, B. Adam, Characterization of Al-7Si-Mg-Cu Turbine Impeller Produced by Investment Casting. Adv. Mat. Research 789 (2013) 324-329.

DOI: 10.4028/www.scientific.net/amr.789.324

Google Scholar

[5] A.M. Kliauga, E.A. Vieira, M. Ferrante, The influence of impurity level and tin addition on the ageing heat treatment of the 356 class alloy. Mat. Sci. Eng. A 480 (2008) 5-16.

DOI: 10.1016/j.msea.2007.07.091

Google Scholar

[6] N. Nafsin, and H.M.M.A. Rashed, Effects of copper and magnesium on microstructure and hardness Al-Cu-Mg alloy. Int. J. Eng. Adv. Tech. 2 (5) (2013) 533-536.

Google Scholar

[7] S.P. Ringer, and K. Hono, Microstructural Evolution and Age Hardening in Aluminium Alloys: Atom Probe Field-Ion Mocroscopy and Transmission Electron Microscopy Studies. Mat. Charact. 44 (2000) 101-131.

DOI: 10.1016/s1044-5803(99)00051-0

Google Scholar

[8] S. Seifeddine, E. Sjolander, T. Bogdanoff, On the Role of Copper and Cooling Rates on the Microstructure, Defect Formation, and Mechanical Properties of Al-Si-Mg Alloy. J. Mat. Sci. App. 4 (2013) 171-178.

DOI: 10.4236/msa.2013.43020

Google Scholar

[9] A. Zulfia, R. Juwita, A. Uliana, Jujur, I Nyoman, J. Raharjo, Proses Penuaan (Aging) pada Paduan Alumunium AA 333 Hasil Proses Sand Casting. Jurnal Teknik Mesin 12 (1) (2010) 13-20.

DOI: 10.9744/jtm.12.1.13-20

Google Scholar

[10] M.J. Starink, and P.V. Mourik. A Calorimetric Study of Precipitation in Al-Cu Alloy with Silicon Particles. Metal. Trans. A 22A (1997) 665-674.

DOI: 10.1007/bf02670289

Google Scholar

[11] L. He, H. Zhang, J. Cui. Effects of pre-ageing treatment on subsequent artificial ageing characteristics of an Al-1.01Mg-0.68Si-1.78Cu Alloy. J. Mater. Sci. Tech. 26 (2) (2010) 141-145.

DOI: 10.1016/s1005-0302(10)60023-0

Google Scholar