Tribocorrosion Behavior of Ti6Al4V Machined and Burnished Components for Biomedical Application

Article Preview

Abstract:

Nowadays, the increased average age of patients and the decreased age at which arthroplasty is carried out represents a reason for the necessity of higher quality standards for prostheses. In particular, tribocorrosion generates an irreversible transformation of the materials and the release of particles and metal ions in toxic concentrations in the biological environment in which the systems are implanted. One of the most used materials for prosthetic implants is the Ti6Al4V alloy but its tribological behavior is still challenging for the application. Employing and optimizing severe plastic deformation processes represents a way to obtain prostheses with superior performance improving patients’ quality of life and reducing the burden on National Health Cares. Ti6Al4V bars have undergone machining with semi-finishing parameters and burnishing processes. Tribocorrosion tests have been performed in a custom-made cylinder-on-disk configuration employing Al2O3 counterparts and phosphate buffer solution with the addition of albumin as simulated body fluid. The effects of sole machining and its combination with burnishing on surface quality and specific wear rate (SWR) have been assessed with respect to as received surface conditions. Optical microscopy, stylus profilometry and sample weighing before tests and at specific intervals during the tests have been employed for characterization. As a main result, it has been found that burnishing process is able to improve SWR of Ti6Al4V samples with respect to both as received and machined samples. Furthermore, the overall behavior of tribological system is gradually improved first employing sole machining and then combining machining and burnishing, reducing SWR of counterparts as well.

You have full access to the following eBook

Info:

* - Corresponding Author

[1] R.J. Ferguson, A.J. Palmer, A. Taylor, M.L. Porter, H. Malchau, S. Glyn-Jones, Hip replacement, Lancet. 392 (2018) 1662–1671. https://doi.org/10.1016/S0140-6736(18)31777-X.

DOI: 10.1016/s0140-6736(18)31777-x

Google Scholar

[2] Y. Jun, K. Choi, Design of patient-specific hip implants based on the 3D geometry of the human femur, Adv. Eng. Softw. 41 (2010) 537–547. https://doi.org/10.1016/j.advengsoft.2009.10.016.

DOI: 10.1016/j.advengsoft.2009.10.016

Google Scholar

[3] M. Merola, S. Affatato, Materials for hip prostheses: A review of wear and loading considerations, Materials (Basel). 12 (2019). https://doi.org/10.3390/ma12030495.

DOI: 10.3390/ma12030495

Google Scholar

[4] M. Choroszyński, M.R. Choroszyński, S.J. Skrzypek, Biomaterials for hip implants - Important considerations relating to the choice of materials, 2017. https://doi.org/10.1515/bams-2017-0017.

DOI: 10.1515/bams-2017-0017

Google Scholar

[5] K.L. Urish, N.J. Giori, J.E. Lemons, W.M. Mihalko, N. Hallab, Trunnion Corrosion in Total Hip Arthroplasty—Basic Concepts, Orthop. Clin. North Am. 50 (2019) 281–288. https://doi.org/10.1016/j.ocl.2019.02.001.

DOI: 10.1016/j.ocl.2019.02.001

Google Scholar

[6] B.J. Kang, Y.C. Ha, D.W. Ham, S.C. Hwang, Y.K. Lee, K.H. Koo, Third-Generation Alumina-on-Alumina Total Hip Arthroplasty: 14 to 16-Year Follow-Up Study, J. Arthroplasty. 30 (2015) 411–415. https://doi.org/10.1016/j.arth.2014.09.020.

DOI: 10.1016/j.arth.2014.09.020

Google Scholar

[7] P. Boutin, P. Christel, J. ‐M Dorlot, A. Meunier, A. de Roquancourt, D. Blanquaert, S. Herman, L. Sedel, J. Witvoet, The use of dense alumina–alumina ceramic combination in total hip replacement, J. Biomed. Mater. Res. 22 (1988) 1203–1232. https://doi.org/10.1002/jbm.820221210.

DOI: 10.1002/jbm.820221210

Google Scholar

[8] V. Schulze, F. Bleicher, P. Groche, Y.B. Guo, Y.S. Pyun, Surface modification by machine hammer peening and burnishing, CIRP Ann. - Manuf. Technol. 65 (2016) 809–832. https://doi.org/10.1016/j.cirp.2016.05.005.

DOI: 10.1016/j.cirp.2016.05.005

Google Scholar

[9] G. Rotella, L. Filice, Surface modifications induced by roller burnishing of Ti6Al4V under different cooling / lubrication conditions, (2019) 9–11.

DOI: 10.1007/978-3-030-57729-2_10

Google Scholar

[10] D.J. Hornbach, P.S. Prevey, E.F. Loftus, Application of Low Plasticity Burnishing (LPB) to improve the fatigue performance of Ti-6AI-4V femoral hip stems, J. ASTM Int. 3 (2006). https://doi.org/10.1520/jai13580.

DOI: 10.1520/jai13580

Google Scholar

[11] G. Rotella, M.R. Saffioti, M. Sanguedolce, D. Umbrello, Finite element modelling of combined turning/burnishing effects on surface integrity of Ti6Al4V alloy, Int. J. Adv. Manuf. Technol. (2021). https://doi.org/10.1007/s00170-021-08219-4.

DOI: 10.1007/s00170-021-08219-4

Google Scholar

[12] M.J. Runa, M.T. Mathew, L.A. Rocha, Tribocorrosion response of the Ti6Al4V alloys commonly used in femoral stems, Tribol. Int. 68 (2013) 85–93. https://doi.org/10.1016/j.triboint.2013.09.022.

DOI: 10.1016/j.triboint.2013.09.022

Google Scholar

[13] H. Mishina, M. Kojima, Changes in human serum albumin on arthroplasty frictional surfaces, Wear. 265 (2008) 655–663. https://doi.org/10.1016/j.wear.2007.12.006.

DOI: 10.1016/j.wear.2007.12.006

Google Scholar

[14] S. Mischler, A.I. Muñoz, Wear of CoCrMo alloys used in metal-on-metal hip joints: A tribocorrosion appraisal, Wear. 297 (2013) 1081–1094. https://doi.org/10.1016/j.wear.2012.11.061.

DOI: 10.1016/j.wear.2012.11.061

Google Scholar

[15] ASTM, G99. Standard Test Method for Wear Testing with a Pin-on-Disk Apparatus, ASTM Int. West Conshohocken, PA. G99 (2016) 1–5. https://doi.org/10.1520/G0099-05R10.2.

Google Scholar

[16] Raymond G. Bayer, Mechanical Wear: Fundamentals and Testing, Second edi, Marcel Dekker, Inc., New York (USA), (2004).

Google Scholar