Abstract:

Magnesium alloys containing Rare Earth elements have proven to be suitable candidates for uses at high temperatures due to their good creep resistance as well as for use in biodegradable implants due to their adequate corrosion rate and biocompatibility. This work investigates the fatigue strength and cyclic deformation behavior of an extruded Mg10Gd1Nd in comparison to Mg10Gd and possible benchmark alloys WE43 and AZ31. The influence of the alloying element Nd is remarkable. The finite life fatigue strengths of Mg10Gd1Nd in the SN-diagram (Wöhler curve) are strongly improved compared to Mg10Gd and almost reach the strength values of WE43. Fracture surface morphology and crack propagation are discussed with attention given to low and high cycle fatigue. The very fine grain size, as the result of dynamic recrystallization during extrusion, offers high elongation at fracture. Therefore the residual fracture surface, where rapid failure occurs, is rather small in the high cycle fatigue samples. The size of the slow crack growth area has been determined by the appearance of benchmark ridges and fatigue striations and is discussed in correlation to stress and number of cycles. Scatter behavior of fatigue life was investigated by optical microcopy. The microstructure consists of second phase alignments in the extrusion direction, which differs in length, precipitate size and distance. Crack branching appears depending on microstructure and the load applied.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 783-786)

Pages:

419-424

Citation:

Online since:

May 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] L. L. Rokhlin: Magnesium alloys containing rare earth elements – structure and properties (Taylor & Francis, London, UK 2003).

Google Scholar

[2] H. Dieringa et al.: Materials Science Forum 690 (2011), pp.270-273.

Google Scholar

[3] N. Hort et al.: Acta Biomaterialia 6 (2010), pp.1714-1725.

Google Scholar

[4] P. Maier et al.: Materials Science Forum 690 (2011), pp.495-498.

Google Scholar

[5] C. Potzies and K.U. Kainer: Adv Eng Mater 6 (2002), pp.281-289.

Google Scholar

[6] U. Noster and B. Scholtes: Mater Sci Forum 419-422 (2003), pp.103-108.

Google Scholar

[7] S. Begum et al.: Int. J. Fatigue 31 (2009), p.726–735.

Google Scholar

[8] Ya. Unigovski et al. Materials Science and Engineering A 360 (2003), pp.132-139.

Google Scholar

[9] Z.Y. Nan et al. Scripta Materialia 50 (2004), pp.429-434.

Google Scholar

[10] S. Xu et al. Canadian Metallurgical Quarterly 44 (2005), pp.155-166.

Google Scholar

[11] M. Huppmann et al.: Materials Science and Engineering A 527 (2010), pp.5514-5521.

Google Scholar

[12] X.N. Gu et al. Acta Biomaterialia 6 (2010), p.4605–4613.

Google Scholar

[13] F.A. Mirza et al.: Materials Science and Engineering A 575 (2003), pp.65-73.

Google Scholar

[14] V. Kree et al. Practical Metallography 41 (2004), pp.233-2346.

Google Scholar

[15] Q. Yu et al.: Int. J. Fatigue 36 (2012), pp.47-58.

Google Scholar

[16] C.L. Mendis et al.: MS&T'13, Magnesium Technology (2013), in press.

Google Scholar