Abstract:

Mechanical spectra of an Al-12.7Si-0.7Mg alloy under extrusion and the solid solution treatment followed artificial aging (T6) states were measured at different frequencies. It has been found that their spectra present differences. There was an obvious internal friction peak near to 200°C with increasing the temperature. The value of internal friction presented increase started from 300°Cand height of the peak was low, there existed a peak near to 270°C during the cooling processes in the spectrum for the extrusion state. For the T6 state alloy, no peaks could be observed during the heating processes. With decreasing the temperature, the internal friction peaks were again observed near 200°C and 270°C.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

182-186

Citation:

Online since:

April 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Matsuura K, Kudoh M, kinoshit A. H.,et al, Precipitation of Si particles in a super rapidly solidified Al-Si hypereutectic alloy, Materials chemistry and physics[J] 2003,81(2/3) :393-395.

DOI: 10.1016/s0254-0584(03)00030-0

Google Scholar

[2] Xiu Z Y,Chen G Q,Wang X F, et al., Microstructure and performance of Al-Si alloy with high Si content by high temperature diffusion treatment, Transactions of Nonferrous metals society of china[J] ,2010,20(11):2134-2138.

DOI: 10.1016/s1003-6326(09)60430-1

Google Scholar

[3] Gupta M, Ling S., Microstructure and mechanical properties of hypo/hyper eutectic Al-Si alloys synthesized using a near net shape forming technique, Journal of alloys and Compounds[J], 1999,287(1/2):284-294.

DOI: 10.1016/s0925-8388(99)00062-6

Google Scholar

[4] Ott R D,Blue C A,Santella M L et al, The influence of a heat treat on the tribological performance of a high wear resistant high Si Al alloy weld overlay. Wear[J] 2001,251:868-874.

DOI: 10.1016/s0043-1648(01)00744-x

Google Scholar

[5] Liu Fang, Yu Fuxiao, Zhao Dazhi,Zhuo Liang, Microstructure and mechanical properties of an Al-12.7Si-0.7Mg alloy processed by extrusion and heat treatment. materials science and engineering A[J], A528(2011)3786-3790.

DOI: 10.1016/j.msea.2011.01.041

Google Scholar

[6] Furong Cao, Zhuoliang Li, Nianxin Zhang Hua Ding,et al, Superplasticity flow and fracture mechanism in an Al-12.7Si-0.7Mg alloy,Materials science and engineering A[J], A571 (2013)167-183.

DOI: 10.1016/j.msea.2013.02.010

Google Scholar

[7] Liu Fang ,Yu Fuxiao, Zhao Dazhi, Zuo Liang,The effect of artificial aging treatment on microstructure and tensile properties of Al-12.7Si-0.7Mg alloy[J].Light metals[J],2012 435-439.

DOI: 10.1002/9781118359259.ch74

Google Scholar

[8] Hong Tao, Gong Yuanping, Tian Ni, Zhao Gang, et al, Effect of solution temperature on microstructure and properties of Al-12.7Si-0.7Mg aluminum alloy extrusion, Chinese journal of rare metals[J],2013 36(3) 368-372.

Google Scholar

[9] Ji Jingwen, Li Shangyi, On the development of internal friction in metallurgy, Physics[J], 1995,24 599-605;

Google Scholar

[10] Kê T. S, Theory foundation of internal friction in Solid: Grain boundary relaxation and Structure[M] Science Press,2000,beijing.

Google Scholar

[11] Kê T. S.,Phys. Rev., 1947,71(8);533-546.

Google Scholar

[12] Nowick A. J. And Berry B. S., Anelastic Relaxation in Crystalline Solids[M], Acad. Press, New York and London,1972 ,P444.

Google Scholar

[13] Ji Jingwen, Yu Ning, the Mechanism of the damping peaks related to internal friction in metallurgy, Progress in physic[J]s,2006,26(34)296-308.

Google Scholar