Influence of Top Slag on the Plasticity of CaO-SiO2-Al2O3 Inclusions in 42CrMoA Crankshaft Steel

Article Preview

Abstract:

In order to control the plasticity of CaO-SiO2-Al2O3 system inclusions so as to reduce the harm to the quality of 42CrMoA crankshaft steel, the target controlling ranges of CaO-SiO2-Al2O3 inclusions is put forward. On the basis, influence of CaO-SiO2-Al2O3 and CaO-SiO2-Al2O3-MgO system top slag on the content of calcium and aluminum in molten steel is contrasted. Theoretical research results show that, calcium activity should be controlled in the range of (90~3300)×10-10, oxygen activity should be below 7×10-6, the mass percent of calcium should be controlled more than 75ppm. And CaO-SiO2-Al2O3-MgO should be a good choice to obtain the plastic inclusions of CaO-SiO2-Al2O3.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

285-288

Citation:

Online since:

October 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2015 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] F. J. Espadafor, J. B. Villanueva, M. T. García: Eng. Fail. Anal., Vol. 16 (2009), p.2333.

Google Scholar

[2] Z.W. Yu and X.L. Xu: Eng. Fail. Anal., Vol. 12(2005), p.487.

Google Scholar

[3] T. Yu: Procedia Earth and Planetary Science (2), p.89.

Google Scholar

[4] G. V. Lasko, Deryugin, YeYe, Schmauder, S.: Comput. Mater. Sci., Vol. 26 (2003), p.20.

Google Scholar

[5] Q.X. Ma, Z.C. Wang Y.X. Zhong: J. Mater. Process. Technol., Vol. 123(2002), p.61.

Google Scholar

[6] H.X. Yu, X.H. Wang, J. Zhang, H.B. Li and W.J. Wang: J. Iron. Steel Res. Int. (2011), p.6. (in Chinese).

Google Scholar

[7] J.X. Chen: Steel Commonly Used Chart Data Book, Metallurgical Industry Press (2010) (in Chinese).

Google Scholar