Porous graphite was synthesized by removal of template after pyrolysis of PFO (pyrolized fuel oil) using kenyaite template with cobalt catalyst. Pyrolysis was conducted for 3-18 hr at 900-1350°C. Porous graphite was synthesized at 900°C after pyrolizing during 3 h. Porous graphite was well crystallized with increasing amount of cobalt. Specific surface area was the range of 274-491 m2/g depending on pyrolysis conditions.