Synthesis of Nanosized Ag0.9Na0.1(Nb0.7Ta0.3)O3 Ceramic Powder and Investigation on its Property

Article Preview

Abstract:

In this communication, Ag0.9Na0.1(Nb0.7Ta0.3)O3(ANNT) mixed oxide powder was synthesized by citrate wet chemical method. TG-DTA, XRD and TEM analyses showed that the reaction temperature was 800°C, the calcining time was three hours, and the product was pure ANNT in well-dispersed grain structure (35nm in average).

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 148-149)

Pages:

1497-1500

Citation:

Online since:

October 2010

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2011 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] A. Kania, et al . J of Crystral Growth, 1989(96), p.703.

Google Scholar

[2] A. Kania, Phase Transition , 1983(3), p.131.

Google Scholar

[3] Toshimi F, Chihiro S.J of Mater Res, 1992, 7(7), p.1883.

Google Scholar

[4] Ravichandran, Meyer R, Roy R et al. Materials Research Bulletin, 1996, 31(7), p.817.

Google Scholar

[5] Daling Lu, Tokumitsu Katou et al. Chemical Mater. 2005, 17, p.632.

Google Scholar

[6] A. Kania, J of Crystral Growth, 1989(96), p.703.

Google Scholar

[7] A. Kania, Phase Transition , 1983(3), p.13.

Google Scholar