The Study of a Kind of New Synthetic Paper Coating Thickness Agent

Article Preview

Abstract:

In this paper, Water glass and sulfuric acid were used as raw materials to do the synthesis of hydrated silica by the method of precipitation, and then hydrated silica is applied in paper coating. By examining the changes of the coated paper’s various properties to study the effects of different reaction conditions to the final products. And then we obtained a optimal synthesis conditions: sulfuric acid concentration 25%, reaction time 50min, reaction temperature 80°C, sodium silicate modulus 2.8, stirring speed 150r/min, the relative amount of sodium sulfate content compared to SiO2 is 25% .And at last the outward appearance of the hydrated silica and the structural changes in paper coating were observed by scanning electron microscopy.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 236-238)

Pages:

1256-1260

Citation:

Online since:

May 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2011 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Xiushan Han.Chemical Engineering Desihgn Communictions,:2005,31(4):46-49.

Google Scholar

[2] Yao Chen,Xinwei Yu,Zhixin Zhong,Jiacong Hu,Yingli Tan.Inorganic Chemicals Industry,2005,37(2):18-20.

Google Scholar

[3] Yishun Cui.Inorganic Chemicals Industry,2006,38(11):21-22.

Google Scholar

[4] Taipeng Hou, Yingkui Liu. .Non-metallic Minerals, 2000,23(1):26-28.

Google Scholar

[5] Qichun Zhang, Qiaoming Ye. Applied Chemistry,1999,16(5):91-93.

Google Scholar

[6] Guang Zhou, Yanji Wang. East China Geological Institute,2001,24(4):298- 302.

Google Scholar