Study on Purification and Removal of Iron from Alloy Anode

Article Preview

Abstract:

Residue of alloy anode generated in three-layer liquid electrolytic purifying method is refined, the state of iron in raw materials is analysed. The state (morphology) changes of iron refined by different refining agent are investigated. Results show: 40% of boron salts or phosphate as the main component of refining agent adding 15% NaCl、20% KCl、15% CaF2、5% NaF、5% cryolite, melting the residue of alloy anode at 1100°C and 1200°C respectively, the crystal could be incubated to grow up fully, it is benefit for collecting iron. When the soaking time is 150min, iron component in alloy is 4.8%,it reaches the standard taking back into the aluminum refining process.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 391-392)

Pages:

883-887

Citation:

Online since:

December 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] F. Mathieux and D. Brissaud: Resource, Conservation and Recycling Vol. 55 (2010), p.92.

Google Scholar

[2] J. L. Wang, S. J. Zhang and Q. Ouyang: Nonferrous Metals Vol. 5 (2004), p.29.

Google Scholar

[3] J. W. Ning and J. Li: Non-ferrous Mining and Metallurgy Vol. 21 (2005), p.1.

Google Scholar

[4] Y. Li: Light-weight MetalS Vol. 11 (2001), p.37.

Google Scholar

[5] V. Kamavaram, D. Mantha and R. G. Reddy: Electrochimica Acta Vol. 50 (2005), p.3286.

Google Scholar

[6] W. Haupin: Encyclopedia Materials: Science and Technology Vol. 14 (2008), p.132.

Google Scholar

[7] S. Lu, K. D. Gu and L. S Zheng: (National Defence Industry Press, Beijing 1983).

Google Scholar