Mechanical Properties and Morphologies of PP/Co-PP/Talc Composites for Microwave Application

Article Preview

Abstract:

Unmodified talc fillers were compounded with polypropylene (PP) and copolymer polyethylene (Co-PP) separately in a Brabender plasticorder internal mixer at 180 °C and 50 rpm in order to obtain composites, which contain 040 phr (per 100 part of resin) of filler at 40 phr intervals. The morphology development and the mechanical properties of the composites with reference to filler loading were investigated. In terms of mechanical properties, Youngs modulus and maximum compression load increased, whereas yield strength and elongation at break decreased with the increase in filler loading of PP/Co-PP/Talc composites. The PP/Co-PP exhibited lower yield strength and youngs modulus, and higher elongation at break than talc composites (data not show here). Scanning electron microscopy (SEM) was used to examine the structure of the fracture surface to justify the variation of the measured mechanical properties.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

711-715

Citation:

Online since:

December 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] F. Dellisanti, G. Valdrè, M. Mondonico : Changes of the main physical and technological properties of talc due to mechanical strain. Applied Clay Science Vol. 42 (2009), p.398.

DOI: 10.1016/j.clay.2008.04.002

Google Scholar

[2] M. Denac, V Musil, I. mit, F. Ranogajec: Effects of talc and gamma irradiation on mechanical properties and morphology of isotactic polypropylene/talc composites. Polymer Degradation and Stability Vol. 82 (2003), p.263.

DOI: 10.1016/s0141-3910(03)00220-9

Google Scholar

[3] Y.W. Leong, M.B. Abu Bakar, Z.A. Mohd Ishak, A. Ariffin: Characterization of talc/calcium carbonate filled polypropylene hybrid composites weathered in a natural environment. Polymer Degradation and Stability Vol. 83 (2004), p.411.

DOI: 10.1016/j.polymdegradstab.2003.08.004

Google Scholar

[4] Md. A. Gafur , R. Nasrin, Md. F. Mina, Md. A.H. Bhuiyan, Y. Tamba, T. Asano: Structures and properties of the compression-molded istactic-polypropylene/talc composites: Effect of cooling and rolling. Polymer Degradation and Stability Vol. 95 (2010).

DOI: 10.1016/j.polymdegradstab.2010.05.001

Google Scholar

[5] M. Longerey, J. -M. Lopez cuesta, P. Gaudon, A. Crespy: Talcs and brominated trimethylphenyl indane/Sb2O3 blend in a PP-PE copolymer. Polymer Degradation and Stability Vol. 64 (1999), p.489.

DOI: 10.1016/s0141-3910(98)00147-5

Google Scholar

[6] H.G.B. Premalal, H. Ismail, A. Baharin: Comparison of the mechanical properties of rice husk powder filled polypropylene composites with talc filled polypropylene composites. Polymer Testing Vol. 21 (2002), p.833.

DOI: 10.1016/s0142-9418(02)00018-1

Google Scholar

[7] A. Wong, C.B. Park: The effects of extensional stresses on the foamability of polystyrene–talc composites blown with carbon dioxide. Chemical Engineering Science, Vol. 75 (2012), pp.49-62.

DOI: 10.1016/j.ces.2012.02.040

Google Scholar

[8] Q. Ding, Z. Zhang, J. Jiang, G. Li, K. Mai: Crystallization behavior and melting characteristics of wollastonite filled β-isotactic polypropylene composites. Thermochimica Acta, Vol. 536 (2012), pp.47-54.

DOI: 10.1016/j.tca.2012.02.023

Google Scholar