The Preparation of Loaded Photocatalyst for Advanced Treatment of NH3-N in Coking Water

Article Preview

Abstract:

Photocatalyst of Fe-Sm-Yb modified TiO2 loaded on clay brick was prepared for degradation of NH3-N in coking water. The influence factors of NH3-N degradation rates were discussed by single factor experiment and orthogonal experiment. The optimum process conditions of photocatalytic degradation NH3-N in coking water were confirmed. The results show that NH3-N degradation rates 82.23% were highest in the conditions of pH 6.5, photocatalyst charge of 1.4 g, illumination for 6h, reaction at 55°C, calcination at 500°C.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 726-731)

Pages:

2829-2832

Citation:

Online since:

August 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Shijun Qiao, Aiping Zhao, Xiaolian Xu, et al. Research of Environmental Sciences. 18(2005), 43-45. ( In Chinese)

Google Scholar

[2] Jianchang Li, Dan Feng, Xianping Luo, et al. Sichuan Nonferrous Metals. 9(2008), 41-44. ( In Chinese)

Google Scholar

[3] Haidong Zhao, Xudong Liu, Chi He. Liaoning Chemical Industry. 38(2009), 783-785. ( In Chinese)

Google Scholar

[4] Zhengfeng Liu, Shouxin Liu, Li Xiaohui, et al. Chemistry Bulletin. 10(2008), 755-764. ( In Chinese)

Google Scholar

[5] Feng Zhang, Miao Li, Wenqi Li, et al. Chemical Engineering Journal. 175(2011), 349-355.

Google Scholar

[6] Marie Faure, Fabien Gerardin, Jean-Claude Andre, et al. Journal of Photochemistry and Photobiology A: Chemistry. 222(2011), 323-329.

Google Scholar

[7] Jingjing Xu. Powder Technology. 210(2011), 1-5.

Google Scholar

[8] Lijuan Xi, Yingjie Zhang, Wenhui Yang, et al. Industrial Water Treatment. 27(2007), 56-58. ( In Chinese)

Google Scholar