Lamination of Green Ceramic Tapes with Adhesive at Ambient Temperature

Article Preview

Abstract:

In this paper, green ceramic tapes are joined together by adhesive based lamination technique. The effects of adhesive concentration, pressure on the lamination and sintering temperature on the laminate are mainly discussed. The parameters are also optimized. It was shown that the effect of adhesive concentration and pressure on the lamination is obvious and the effect of sintering temperature is not big. 10 layers of cordierite tapes can be laminated under 2MPa with a dwell time of 3min with PVA by adhesive based lamination. The adhesive based lamination can be used to be an alternative of thermo-compressive lamination.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 774-776)

Pages:

716-719

Citation:

Online since:

September 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] R.E. Mistler: Am. Ceram. Soc. Bull, Vol. 69(1990), pp.1022-1026.

Google Scholar

[2] T. Chartier, T. Rouxel: J. Euro. Ceram. Soc, Vol. 17(1997), 299-308.

Google Scholar

[3] A. Roosen: J. Eur. Ceram. Soc, Vol. 21(2001), p.1993-(1996).

Google Scholar

[4] Z.M. Rocha, N. Ibañez Garcia, N.A. Oliveira, et al: Proceedings of IMAPS Conference and exhibition on Ceramic Interconnect Technology, Denver (2004).

Google Scholar

[5] J. Gurauskis, A.J. Sanchez-Herencia, C. Baudin: J. Euro. Ceram. Soc, Vol. 27 (2007), pp.1389-1394.

Google Scholar