Alignment of the Microstructure of Castings from the Heterophase Lead Bronzes

Article Preview

Abstract:

This paper reports on the use of nanopowders in the coating composition forms in casting blanks from lead bronzes for the petrochemical industry. Influence of composition of used protective separating coating of casting mold on the microstructure castings was investigated. For experimental investigations following coating were selected [1]: the mixture of zirconium dioxide nanopowder with industrial oil and the same composition as it’s, but on the basis of aluminum oxide nanopowder. As the test material multicomponent and lead bronzes were selected. The cooling curves castings using coatings of different compositions by means the developed device thermograph were constructed using techniques developed by the authors. The study results showed that the greatest reduction in the cooling rate at the time of crystallization bronze corresponds to coating casting mold based on powder of zirconium dioxide (45 °C/c). The cooling rate is reduced only to 65 °C/c when coating based on aluminum oxide. Decrease the cooling rate of castings using these coatings can change the shape and size of lead inclusions and align the casting structure in section. Form inclusions lead is becoming more spherical and their interfacial surface is leveled. The greatest changes occur in the surface layers of castings. Is shown that the multicomponent bronzes decreased speed the cooling due to the use plasters leads not only to changes in the morphology of inclusions but also to lead the change in the phase composition. Decrease of cooling rate leads to increasing the amount of eutectoid and growth of hardness casting.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

163-167

Citation:

Online since:

January 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] N.V. Martyushev, Yu.P. Egorov, Determination of the signal strength with the computer analysis of the material structure, in Proceedings of the 9th International Scientific and Practical Conference of Students, Post-graduates and Young Scientists - Modern Techniques and Technologies, MTT' 2003, Tomsk Polytechnical University, Tomsk, 2003, p.192.

DOI: 10.1109/spcmtt.2003.1438190

Google Scholar

[2] D. Empl, V. Laporte, E. Vincent, N. Dewobroto, A. Mortensen, Improvement of elevated temperature mechanical properties of Cu–Ni–Sn–Pb alloys, Materials Science and Engineering A. 527 (2010) 4326–4333.

DOI: 10.1016/j.msea.2010.03.056

Google Scholar

[3] Ugur Ozsarac, Fehim Findik, Mehmet Durman, The wear behaviour investigation of sliding bearings with a designed testing machine, Materials and Design. 28 (2007) 345–350.

DOI: 10.1016/j.matdes.2005.05.017

Google Scholar

[4] N.V. Martyushev, Leaded-tin bronze destruction mechanism, in Proceedings - 2012 7th International Forum on Strategic Technology, IFOST 2012, Tomsk Polytechnical University, Tomsk, 2012, vol. 1, p.192–194.

DOI: 10.1109/ifost.2012.6357597

Google Scholar

[5] A.P. Babichev, N.A. Babushkina, A.M. Bratkovskiy et al, Physical magnitudes : reference book, Energoatomizdat, Moscow, (1991).

Google Scholar

[6] A.V. Korchmit, Yu.P. Egorov, Technique of bronze cooling speed determination, Metal Processing. 1 (2005) 23–25.

Google Scholar

[7] N.V. Martjushev, E.N. Pashkov, Tribotechnical properties lead bronzes, Applied Mechanics and Materials. 379 (2013) 87-90.

DOI: 10.4028/www.scientific.net/amm.379.87

Google Scholar

[8] N.V. Martyushev, E.N. Pashkov, Bronze sealing rings defects and ways of its elimination, Applied Mechanics and Materials. 379 (2013) 82-86.

DOI: 10.4028/www.scientific.net/amm.379.82

Google Scholar